MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Petrothene GA501152 Linear Low Density Polyethylene (LLDPE), Film Grade  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade

Material Notes: The Petrothene GA501 series of resins is pelletized liner low density polyethylene selected for film extrusion applications that require excellent drawdown and toughness. These resins have excellent puncture resistance, elongation and heat seal strength. Typical applications include heavy duty shipping sacks, trash can liners, commercial and industrial packaging, as well as food and consumer packaging. GA501 is available without additives or fully formulated with slip and antiblock additives. Applications: Agriculture Film, Bags & Pouches, Can Liners, Film Wrap, Food Packaging Film, Heavy Duty Packaging, Lamination Film, Liner Film, Retail Carryout Bags, Shrink Film.

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Base Resin Density 0.918 g/cc0.0332 lb/in³ASTM D1505
Density 0.925 g/cc0.0334 lb/in³ASTM D1505
Melt Flow 1.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
1.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Antiblock Level 10000 ppm10000 ppmLYB Method
Slip Level 1000 ppm1000 ppmLYB Method
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 580 %580 %ASTM D882
Film Elongation at Break, TD 725 %725 %ASTM D882
Elmendorf Tear Strength MD 125 g125 gASTM D1922
Elmendorf Tear Strength TD 330 g330 gASTM D1922
Dart Drop Test 100 g0.221 lbF50; ASTM D1709
Film Tensile Strength at Break, MD 45.5 MPa6600 psiASTM D882
Film Tensile Strength at Break, TD 32.4 MPa4700 psiASTM D882
1% Secant Modulus, MD 186 MPa27000 psiASTM D882
1% Secant Modulus, TD 193 MPa28000 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 107 °C225 °FASTM D1525
 
Processing PropertiesMetricEnglishComments
Melt Temperature 204 - 232 °C400 - 450 °F1.5 to 3.0:1 blow up ratio
 
Descriptive Properties
Polymer Processing AidPresent, LYB Method
Processing MethodBlown Film
Test Specimen1.0 mil gauge, 2.5:1 BUR

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Total Lumicene® mPE M 2735 S01 Metallocene Polyethylene, Cast Film
Total Lotrene® Q2018N Linear Low Density Polyethylene, Cast Film
Total Lotrene® Q2018H Linear Low Density Polyethylene, Blown Film
Total Lotrene® Q1018H Linear Low Density Polyethylene, Blown Film
Total LLDPE LL 1820 Linear Low Density Polyethylene - Blown Film

PEQT8819 / 220453

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.