MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BYK PRIEX® Ionomer 48101 PP random copolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes:
    Ionomers will be used to
  • Strengthen rigidity and hardness while maintaining impact resistance in polyolefins
  • Maintain adhesion even under contaminated conditions especially in fatty substrates
  • Reduce thickness in multi-layer films or pipes
  • Increase elongation resistance in polyolefin fibers
  • Act as a nucleating agent in polyolefins
  • Enhance creep resistance in pipes
  • Reinforce strain hardening in polyolefins
  • Improve compatibility between different polymers
  • Increase oxidation resistance in polyolefins

Former Addcomp product line, acquired by BYK.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 27.0 MPa
Elongation at Break >= 600 %
Tensile Modulus 800 - 900 MPa
 
Thermal PropertiesOriginal ValueComments
Melting Point 135 - 137 °C
Crystallization Temperature 93.0 - 97.0 °C
Deflection Temperature at 0.46 MPa (66 psi) 77.0 °C
 
Descriptive Properties
Oxygen induction time>80 min

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow Surlyn® 9945 Thermoplastic Ionomer Resin
Dow Surlyn® 8920 Ionomer Resin, Sodium
Overview of materials for Ionomer, Film Grade
Overview of materials for Ionomer, Molded
E-Polymers EFLEX® I2030 Ionomer

PPADDC15 / 130327

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.