MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lanxess Addolink® 30/10 technical ground Crosslinking Agent
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Product Information: Addolink® 30/10 technical ground is used in combination with Addolink TT for the production of hard polyurethane rubber qualities. Addolink® 30/10 is noted for its high degree of purity. Thus reduces undesired side reactions. With Addolink® 30/10 molded parts display a high degree of heat resistance and a low compression set. Depending on the used quantity a hardness value between Shore A 84 and Shore D 70 could be reached.

Function: Crosslinking agent for isocyanate crosslinkable polyurethane rubber.

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.14 g/cc
@Temperature 120 °C
0.0412 lb/in³
@Temperature 248 °F
Water Absorption <= 0.20 %<= 0.20 %
Viscosity 7.0 - 10 cP
@Temperature 125 °C
7.0 - 10 cP
@Temperature 257 °F
 
Thermal PropertiesMetricEnglishComments
Melting Point 104 °C219 °F
Flash Point 214 °C417 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
Appearancefine grayish white powder
Hydroxyl value560 mg KOH/g

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLANY8207 / 208600

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.