MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Syensqo (Solvay Specialty Polymers) Zeniva® ZA-520 Resin PEEK, Implantable Grade
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK)

Material Notes: Zeniva® ZA-520 is a grade of polyetheretherketone (PEEK) offered for use in implantable devices. This grade of Zeniva® PEEK is an Image Contrast grade, offering a level of opacity for imaging techniques such as MRI, CT and X-ray. The manufacturing facility for Zeniva® PEEK in Alpharetta, GA is ISO 13485 registered and the relevant aspects of current Good Manufacturing Practices are also applied.

The biomaterial manufacturing processes are carefully validated, and enhanced controls provide product traceability. In addition, all materials are tested in a lab that is ISO 17025 accredited.

The chemical, physical and mechanical properties of finished parts are related to the processes utilized in producing the finished part, for example, molding, machining, annealing, sterilization, etc.

Zeniva® ZA520 is available in resin pellets and rods.

Applications: Body Implants; Medical/Healthcare Applications

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.35 g/cc0.0488 lb/in³ASTM D792
Viscosity 440 cP
@Shear Rate 1000 1/s,
Temperature 400 °C
440 cP
@Shear Rate 1000 1/s,
Temperature 752 °F
Melt; ASTM D3835
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break >= 70.0 MPa>= 10200 psiASTM D638
Tensile Strength, Yield >= 90.0 MPa>= 13100 psiASTM D638
Elongation at Break >= 5.0 %>= 5.0 %ASTM D638
Elongation at Yield >= 4.0 %>= 4.0 %ASTM D638
Tensile Modulus >= 3.30 GPa>= 479 ksiASTM D638
Flexural Yield Strength >= 110 MPa>= 16000 psiASTM D790
Flexural Modulus >= 3.00 GPa>= 435 ksiASTM D790
Izod Impact, Notched >= 0.500 J/cm>= 0.937 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Melting Point 340 °C644 °FPeak; ASTM D3418
Crystallization Temperature 290 °C554 °FPeak; ASTM D3418
Glass Transition Temp, Tg 150 °C302 °FASTM E1356
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 North America
Cytotoxicity - ISO 10993:5Pass
FormsPellets; Rod
Physiochemical Testing - ISO 10993:18Pass

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSOL8Y4639 / 280439

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.