MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
PlastiComp Complet® LCF40 - ETPU Rigid Thermoplastic Polyurethane, 40% Long Carbon Fiber Reinforced  (discontinued **)
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Carbon Fiber Reinforced

Material Notes: Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.

Polyurethane with 40% carbon fiber reinforcement

Information provided by PlastiComp, Inc.

Key Words: Complet® Long Fiber LCF
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.38 g/ccASTM D-792
Filler Content 40 %Carbon Fiber
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 262 MPaASTM D-638
Elongation at Break 1.0 - 2.0 %ASTM D-638
Tensile Modulus 28966 MPaASTM D-638
Flexural Strength 428 MPaASTM D-790
Flexural Modulus 28276 MPaASTM D-790
Izod Impact, Notched 294 J/mASTM D-256
Izod Impact, Unnotched 1121.4 J/mASTM D-4812
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 113 °CASTM D-648
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 400 - 440 °F
Middle Barrel Temperature 410 - 450 °F
Front Barrel Temperature 420 - 460 °F
Nozzle Temperature 430 - 470 °F
Melt Temperature 420 - 460 °F
Mold Temperature 190 °F
Injection Velocity 2.00 - 3.00 in/sec
Drying Temperature 88.0 °C
@Time 14400 sec
Moisture Content <= 0.020 %
Back Pressure 25.0 - 50.0 psi
Cushion 0.250 in
Screw Speed 30 - 50 rpm
 
Descriptive Properties
Injection PressureMedium to maximum

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro Desmopan® 85085A DPS 055 TPU
Covestro Desmopan® 453 Urethane Thermoplastic Elastomer
RTP Company RTP 2381 A Rigid Thermoplastic Polyurethane (RTPU), Carbon Fiber
NYC YT3WBQ Y2O3 CIP (Cold Isostatic Pressing) Granules
Lubrizol Advanced Materials PEARLCOAT® 126K Thermoplastic Polyurethane Elastomer

PPLASTI919 / 159330

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.