SMC 0420 is a low density Premium Class-A SMC for exterior body applications on cars, LCV´s and trucks. These compounds mould to light weight parts with good up to excellent surface quality for body panels with in-line and off-line painting at standard paint bake (100- 140 °C) temperatures. The product complies with all regulations of the automotive industry including low C-emissions. Surface defects like waviness, fibre patterns and orange peel are not existent with this product. To achieve the highest surface quality, we recommend that tool surfaces are mirror polished. The product shows very good adhesion to paint or In Mould Coating (IMC).Information Provided by Menzolit |