MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
ASI® MP 54216 CL Epoxy Adhesive
Categories: Polymer; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: MP54216CL is a two part mineral filled epoxy adhesive designed for bonding metals and plastics. It cures at room temperature to a tough, semi-flexible material. It has good wetting to most surfaces and is free flowing to penetrate cavities and give good self leveling and air release. This product gives very good vibration and impact resistance. It gives good resistance to water, salt spray, inorganic acids and bases and most organic solvents. It was formulated to a 1A:1B volume mix ratio for use in side-by-side dispensing cartridges and meter/mix and dispense equipment. MP54216CL will reach handle cure at room temperature within 16 – 24 hours. Cure time can be accelerated by the application of heat. Times and temperatures from 2 hours at 65°C to 20 minutes at 100°C are typical for most applications. Time to heat substrate must be taken into account. Cooler temperatures will also extend work time and increase cure times.

Information provided by Adhesive Systems, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.31 g/cc
@Temperature 25.0 °C
part B
 1.32 g/cc
@Temperature 25.0 °C
mixed
 1.34 g/cc
@Temperature 25.0 °C
part A
Viscosity 80000 cP
@Temperature 25.0 °C
part A
 80000 cP
@Temperature 25.0 °C
part B
 80000 cP
@Temperature 25.0 °C
mixed
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 70
@Temperature 25.0 °C
Tensile Strength 1800 psi
@Temperature 25.0 °C
Elongation at Break 60 %
Adhesive Bond Strength 3000 psiLap Shear; Al to Al
Peel Strength 25.0 pli
@Temperature 25.0 °C
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 8.00e+13 ohm-cm
@Temperature 25.0 °C
Dielectric Constant 4.5
@Frequency 100 Hz,
Temperature 25.0 °C
Dielectric Strength 410 V/mil
@Temperature 25.0 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 50.0 µm/m-°C
@Temperature <=16.0 °C
 150 µm/m-°C
@Temperature >=16.0 °C
Maximum Service Temperature, Air 150 °C
Minimum Service Temperature, Air -60.0 °C
Glass Transition Temp, Tg 16.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 1.00 hour
@Temperature 60.0 °C
 24.0 - 72.0 hour
@Temperature 25.0 °C
Pot Life 60.0 min
@Temperature 25.0 °C
100 grams
Shelf Life 12.0 Month
 
Descriptive Properties
Color / appearanceclear
Mix Ratio1:1 by volume (Part A to B)
 103:100 by weight (Part A to B)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PASINC9095 / 233462

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.