Base Polymer: Polycarbonate Filler/Additive System: special filler, UV stabilized Special Features: translucent, high light diffusion, light scattering Market Segment: Automotive, Lighting Application Area: lighting, light transparent components, injection molded parts Typical Applications: lamp covers, display elements, operating elements Information provided by Albis Plastics |