MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LyondellBasell Hifax Hostacom TRC 770P NATURAL Thermoplastic Olefinic Elastomer  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Olefinic Elastomer (TPO)

Material Notes: Hifax polypropylene resins based on the Catalloy process are used in applications such as building and construction (e.g., single-ply roofing), industrial applications (e.g., wire and cable), and automotive industries. Hifax priovides good processability, excellent impact resistance, a broad range of stiffness from very soft to rigid products, high temperature resistance and low linear coefficient of thermal expansion.

Hostacom TRC 770P NATURAL high melt flow, 1,600 MPa flexural modulus, UV-stabilized, mineral-filled, precolored thermoplastic elastomeric olefin (TEO) resin has an excellent balance of properties and processability. It is typically used for molded-in color interior automotive applications.

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.02 g/ccMethod A; ISO 1183-1
Melt Flow 28 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 19.0 MPaISO 527-1,-2
Elongation at Yield 7.0 %ISO 527-1,-2
Flexural Modulus 1600 MPaISO 178
Izod Impact, Notched (ISO) 5.80 kJ/m²
@Temperature -30.0 °C
ISO 180
 32.0 kJ/m²
@Temperature 23.0 °C
ISO 180
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 95.0 °Cunannealed; ISO 75B-1,-2
 
Descriptive Properties
Processing MethodInjection Molding

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Hostacom 5106 BLACK Polypropylene, glass fiber reinforced
LyondellBasell Hostacom 1257 BLACK Polypropylene, 22% Talc Filled
LyondellBasell Hifax Hostacom TRC 103P D72926 Polypropylene , Talc Filled
LyondellBasell Hifax Hostacom EYC 2135Y BLACK Polypropylene , Talc Filled
LyondellBasell Dexflex 711-300 BLK Thermoplastic Polyolefin

PEQT7581 / 219218

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.