MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Barlog Plastics KEBATER B511T PBT unreinforced, super tough
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Impact Grade

Material Notes: PBT-I

Information provided by BARLOG plastics GmbH.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.23 g/cc0.0444 lb/in³ISO 1183
Moisture Absorption at Equilibrium 0.20 %0.20 %similar to ISO 62 test
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 40.0 MPa5800 psiISO 527-1
Elongation at Break 50 %50 %ISO 527-1
Tensile Modulus 1.80 GPa261 ksiISO 527-1
Charpy Impact Unnotched  NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179-1eU
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179-1eU
Charpy Impact, Notched 5.00 J/cm²23.8 ft-lb/in²ISO 179-1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+17 ohm-cm1.00e+17 ohm-cmIEC 60093
Surface Resistance 1.00e+13 ohm1.00e+13 ohmIEC 60093
Dielectric Strength 26.0 kV/mm660 kV/inIEC 60243-1
 
Thermal PropertiesMetricEnglishComments
Melting Point 225 °C437 °F10°C/min; ISO 11357-1/-3
Flammability, UL94 HB
@Thickness 0.800 mm
HB
@Thickness 0.0315 in
IEC 60695-11-10
 
Descriptive Properties
Resin TypePBT-I

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Barlog Plastics KEBATER B510 PBT unreinforced
Barlog Plastics KEBATER BF110 PBT, 10% glass fiber reinforced
A. Schulman VOLOY™ 462 Hybrid Reinforced PBT Alloy
Barlog Plastics KEBATER BF230 PBT, 30% glass fiber reinforced, food grade
Barlog Plastics KEBATER BF115 PBT, 15% glass fiber reinforced

PBARLO838 / 149856

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.