Baynat 0759 BX Isocyanate is a low to medium functionality polymeric diphenylmethane diisocyanate (PMDI) with a moderately high 2,4 ’-MDI isomer content. Properties / Applications: Baynat 0759 BX Isocyanate is used in a box pour process to produce sheets of formable rigid foam. The foam sheet is used as the lightweight core material for composite PU headliners. As with any product, use of Baynat 0759 BX Isocyanate in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability. Information provided by Covestro |