MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Polycasa PETG
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); PETG Copolyester

Material Notes: QUINN PETG has good optical properties and a brilliant surface. The PETG range of sheets are easy to fabricate, to vacuum form, and show exceptional low temperature performance. Important benefits of QUINN PETG are its very good chemical resistance and very high impact properties. QUINN PETG meets all current food contact legislation and can be used in contact with unwrapped food. QUINN PETG also combines the following excellent properties: easy to vacuum form, needs no predrying, exceptional low temperature performance, low water absorption, ease to recycle, and very high impact properties
  • Bus shelters
  • Poster glazing
  • Machine guards
  • Medical appliance packaging
  • Displays & signs for external use
  • Refrigerators and cold storeroom equipment
  • Bicycle safety helmets
  • Food containers
  • Lenticular lenses
  • Graphic Arts Lighting controllers for hazardous areas<./li>

Quinn Manufacturing Group rebranded its Plastics Division as Polycasa in 2013.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.27 g/ccASTM D1595
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 105ASTM D785
Tensile Strength at Break 50.0 MPaDIN 53455
Elongation at Break 54 %DIN 53466
Tensile Modulus 2.20 GPaDIN 53455
Flexural Strength 70.0 MPaDIN 53452
Flexural Modulus 2.075 GPaDIN 53452
Izod Impact, Notched (ISO) 11.5 kJ/m²ISO 180
Charpy Impact Unnotched NBDIN 53453
Charpy Impact, Notched 1.00 J/cm²DIN 53453
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cmASTM D257
Surface Resistance >= 1.00e+16 ohmASTM D257
Dielectric Constant 2.6
@Frequency 100 Hz
Dielectric Strength 16.0 kV/mmD149
Dissipation Factor 0.010
@Frequency 50 Hz
IEC 250
 
Thermal PropertiesOriginal ValueComments
CTE, linear 68.0 µm/m-°C
@Temperature 20.0 °C
DIN 53752
Specific Heat Capacity 1.10 J/g-°CASTM D2766
Thermal Conductivity 0.200 W/m-KDIN 52612
Maximum Service Temperature, Air 70.0 °C
Deflection Temperature at 0.46 MPa (66 psi) 68.0 °CDIN 53461
Deflection Temperature at 1.8 MPa (264 psi) 72.0 °CDIN 53461
Vicat Softening Point 82.0 °CDIN 53460
Decomposition Temperature >= 280 °C
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.57DIN 53491
Haze <= 1.0 %ASTM D1003
Transmission, Visible 88 %DIN 5036-3
 
Processing PropertiesOriginal ValueComments
Processing Temperature 120 - 160 °CSheet Forming

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for PETG Copolyester
Eastman Eastar GN071 Natural PETG Copolyester
Plaskolite Mustang PETG Sheet
Plaskolite Vivak PETG Sheet
Changzhou Jinlibao GETAILONG JLB-110900 Clear PETG sheet

PSF0238 / 66589

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.