LG Chemical RS800M ABS, High Modulus, Chemical Resistance to HCFC
Categories:
Polymer
;
Thermoplastic
;
ABS Polymer
;
Acrylonitrile Butadiene Styrene (ABS), Extruded
Material Notes:
Feature: Extrusion Molding, High Modulus, Chemical Resistance to HCFC
Application: Refrigerator Inner Liner
CAS No. 9003-56-9
Information provided by LG Chemical
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Specific Gravity
1.04
g/cc
1.04
g/cc
ASTM D792
Maximum Moisture Content
0.010
0.010
Extrusion Molding
Linear Mold Shrinkage, Flow
0.0040
-
0.0070
cm/cm
@Thickness 3.20 mm
0.0040
-
0.0070
in/in
@Thickness 0.126 in
ASTM D955
Melt Flow
6.0
g/10 min
@Load 10.0 kg,
Temperature 220 °C
6.0
g/10 min
@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Mechanical Properties
Metric
English
Comments
Hardness, Rockwell R
100
100
ASTM D785
Tensile Strength, Yield
44.1
MPa
@Thickness 3.20 mm
6400
psi
@Thickness 0.126 in
50 mm/min; ASTM D638
Elongation at Break
35 %
@Thickness 3.20 mm
35 %
@Thickness 0.126 in
50 mm/min; ASTM D638
Elongation at Yield
>= 5.0 %
@Thickness 3.20 mm
>= 5.0 %
@Thickness 0.126 in
50 mm/min; ASTM D638
Flexural Yield Strength
72.6
MPa
@Thickness 3.20 mm
10500
psi
@Thickness 0.126 in
15 mm/min; ASTM D790
Flexural Modulus
2.40
GPa
@Thickness 3.20 mm
348
ksi
@Thickness 0.126 in
15 mm/min; ASTM D790
Izod Impact, Notched
3.43
J/cm
@Thickness 6.40 mm,
Temperature 23.0 °C
6.43
ft-lb/in
@Thickness 0.252 in,
Temperature 73.4 °F
ASTM D256
3.92
J/cm
@Thickness 3.20 mm,
Temperature 23.0 °C
7.35
ft-lb/in
@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
Electrical Properties
Metric
English
Comments
Hot Wire Ignition, HWI
15
-
30
sec
@Thickness >=1.50 mm
15
-
30
sec
@Thickness >=0.0591 in
30
-
60
sec
@Thickness >=3.00 mm
30
-
60
sec
@Thickness >=0.118 in
High Amp Arc Ignition, HAI
>=
120
arcs
@Thickness 1.50 mm
>=
120
arcs
@Thickness 0.0591 in
>=
120
arcs
@Thickness 3.00 mm
>=
120
arcs
@Thickness 0.118 in
High Voltage Arc-Tracking Rate, HVTR
10.0
-
25.4
mm/min
0.394
-
1.00
in/min
Thermal Properties
Metric
English
Comments
Deflection Temperature at 0.46 MPa (66 psi)
96.0
°C
@Thickness 6.40 mm
205
°F
@Thickness 0.252 in
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi)
89.0
°C
@Thickness 6.40 mm
192
°F
@Thickness 0.252 in
Unannealed; ASTM D648
Vicat Softening Point
96.0
°C
@Load 5.00 kg
205
°F
@Load 11.0 lb
50°C/h; ASTM D1525
UL RTI, Electrical
60.0
°C
@Thickness >=1.50 mm
140
°F
@Thickness >=0.0591 in
UL 746B
60.0
°C
@Thickness >=3.00 mm
140
°F
@Thickness >=0.118 in
UL 746B
UL RTI, Mechanical with Impact
60.0
°C
@Thickness >=1.50 mm
140
°F
@Thickness >=0.0591 in
UL 746B
60.0
°C
@Thickness >=3.00 mm
140
°F
@Thickness >=0.118 in
UL 746B
UL RTI, Mechanical without Impact
60.0
°C
@Thickness >=1.50 mm
140
°F
@Thickness >=0.0591 in
UL 746B
60.0
°C
@Thickness >=3.00 mm
140
°F
@Thickness >=0.118 in
UL 746B
Flammability, UL94
HB
@Thickness >=1.50 mm
HB
@Thickness >=0.0591 in
HB
@Thickness >=3.00 mm
HB
@Thickness >=0.118 in
Processing Properties
Metric
English
Comments
Zone 1
180
-
210
°C
356
-
410
°F
Extrusion Molding
Zone 2
190
-
230
°C
374
-
446
°F
Extrusion Molding
Zone 3
200
-
250
°C
392
-
482
°F
Extrusion Molding
Zone 4
200
-
250
°C
392
-
482
°F
Extrusion Molding
Adapter Temperature
200
-
250
°C
392
-
482
°F
Extrusion Molding
Die Temperature
200
-
250
°C
392
-
482
°F
Extrusion Molding
Melt Temperature
200
-
250
°C
392
-
482
°F
Extrusion Molding
Roll Temperature
60.0
-
90.0
°C
140
-
194
°F
Bottom, Extrusion
70.0
-
90.0
°C
158
-
194
°F
Middle, Extrusion
70.0
-
100
°C
158
-
212
°F
Top, Extrusion
Drying Temperature
70.0
-
80.0
°C
158
-
176
°F
Extrusion Molding
Dry Time
3.00
-
4.00
hour
3.00
-
4.00
hour
Extrusion Molding
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
PLAY040 / 148048
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.