MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Röhm Acrylite® FF Acrylic Sheet  (discontinued **)
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, Optical Sheet

Material Notes: Data provided by CYRO Industries

Continuously manufactured sheet, weather resistant, easy to fabricate. Used in skylights, RVs, boat, motorcycle, and snowmobile fairings, signs, displays, and boutique items.

Information Provided by Evonik CYRO. The former Evonik Methacrylates business has been sold to Röhm (Roehm) GmbH.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.19 g/ccASTM D792
Water Absorption 0.20 %24 hrs, 23°C; ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Hardness, Barcol 48ASTM D2583
Hardness, Rockwell M 93ASTM D785
Tensile Strength, Ultimate 69.0 MPaASTM D638
Elongation at Break 4.5 %ASTM D638
Tensile Modulus 2.80 GPaASTM D638
Flexural Yield Strength 117 MPaASTM D790
Flexural Modulus 3.30 GPaASTM D790
Compressive Yield Strength 117 MPaASTM D695
Izod Impact, Notched 0.220 J/cmASTM D256
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1.00e+16 ohm-cmASTM D257
Surface Resistance 1.00e+15 ohmASTM D257
Dielectric Constant 2.8
@Frequency 1e+6 Hz
ASTM D150
 3.6
@Frequency 60 Hz
ASTM D150
Dielectric Strength 17.0 kV/mm
@Thickness 3.20 mm
Short Time; ASTM D149
Dissipation Factor 0.020
@Frequency 1e+6 Hz
ASTM D150
 0.060
@Frequency 60 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 68.0 µm/m-°C
@Temperature 20.0 °C
ASTM D696
Specific Heat Capacity 1.47 J/g-°C
Thermal Conductivity 0.190 W/m-KCenco-Fitch test
Maximum Service Temperature, Air 71.0 °CContinuous service temperature
 88.0 °CShort-term
Deflection Temperature at 1.8 MPa (264 psi) 91.0 °CASTM D648
Vicat Softening Point 115 °CASTM D1525
Minimum Service Temperature, Air -34.0 °C
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.49ASTM D542
Transmission, Visible 92 %ASTM D1003
 
Processing PropertiesOriginal ValueComments
Processing Temperature 143 - 159 °Cforming temperature

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Röhm ACRYLITE® Extruded Acrylic Sheet
Röhm Acrylite® GP Acrylic Sheet, Cast
Mitsubishi Chemical Advanced Materials Acetron® GP Copolymer Acetal, Porosity-Free, Unfilled, Extruded (ASTM datasheet)
Röhm Acrylite® 8N Acrylic Polymer
Chi Mei Acryrex® CM-205 PMMA

PCYR35 / 29174

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.