MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Norplex-Micarta NP180 Synthetic Fabric  (discontinued **)
Categories: Polymer; Thermoset; Aramid; Epoxy; Filled/Reinforced Thermoset

Material Notes: Description: aramid fabric material with a high performance epoxy resin matrix. Excellent electrical and mechanical properties at elevated temperatures and in adverse environments.

Thickness Tested: 0.062", 0.125", and 0.500"

Key Words: Micarta
Vendors: Norplex-Micarta is the leading manufacturer of high performance thermoset composite materials. We work directly with customers to manufacture the highest quality specialty sheet products, pre-pregs, rods and molded shapes, and tubes to meet demanding composite applications for our OEMs and fabricators around the world. Visit norplex-micarta.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.40 g/cc
Moisture Absorption at Equilibrium 0.31 %
@Thickness 1.57 mm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 80 - 100
@Thickness 1.57 mm
Tensile Strength, Yield 58000 psi
@Thickness 3.17 mm
CW
 62000 psi
@Thickness 3.17 mm
LW
Flexural Strength 56000 psi
@Thickness 1.57 mm
CW
 56000 psi
@Thickness 1.57 mm
LW
Compressive Strength 79000 psi
@Thickness 12.7 mm
Flatwise
Izod Impact, Unnotched 8.00 ft-lb/in
@Thickness 12.7 mm
CW, E-48/50
 10.9 ft-lb/in
@Thickness 12.7 mm
LW, E-48/50
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 3.91
@Thickness 1.57 mm
Cond D-24/23
Dielectric Strength 500 V/mil
@Thickness 1.57 mm
D-48/50
 650 V/mil
@Thickness 1.57 mm
Condition - A
Dielectric Breakdown 47000 V
@Thickness 1.57 mm
Condition A
 54000 V
@Thickness 1.57 mm
D-48/50
Dissipation Factor 0.0275
@Thickness 1.57 mm
Cond D-24/23
Arc Resistance 121 sec
@Thickness 3.17 mm
ASTM D495
 
Thermal PropertiesOriginal ValueComments
CTE, linear 36.3 µm/m-°C
@Thickness 1.57 mm,
Temperature 40.0 - 105 °C
x-axis
 262 µm/m-°C
@Thickness 1.57 mm,
Temperature 105 - 155 °C
x-axis
Maximum Service Temperature, Air 180 °C
Glass Transition Temp, Tg 145 °CTg
Flammability, UL94 V-0

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Polycarbonate, Aramid Fiber Reinforced
Overview of materials for Diallyl Phthalate (DAP) Molding Compound, Long Glass Fiber Filled
Overview of materials for Acetal Copolymer, Aramid Fiber Filled
Norplex-Micarta NP159 Synthetic Fabric
Nanocyl PREGCYL™ NC R2HM-01 Pre-impregnated UD/Fabric Carbon Fibers

PNORPN560 / 48145

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.