Production Method: Aluminum Hydroxychloride is a waste product of the process of benzene alkylation with olefin, obtained through washing out the reaction mass from complex catalyst with chloride aluminum solutions. Applications: Intended for use as a coagulant in the process of industrial wastewater purification and also as an agent for carbon deposits. Information Provided by Kazanorgsintez |