MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Teijin PYROMEX® Poly-acrylonitrile Continuous Filament Tow
Categories: Carbon; Carbon Fiber/Carbon Fibre

Material Notes: Pyromex® is a family of oxidized poly-[acrylonitrile] (PAN) fibers. These fibers have a Limiting Oxygen Index (L.O.I.) of between 50 - 60% oxygen, making Pyromex® much more flame resistant than many other organic fibers such as PBI® (41%), Nomex® (30%), or Kevlar® (28%). For carbon/carbon applications, the low sodium content of these fibers may aid in processing and performance.

Information provided by Teijin Carbon America, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.39 - 1.43 g/cc
Moisture Absorption 4.0 - 10 %
Filament Diameter 14 µm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength >= 230 MPaDry
Elongation at Break >= 15 %Dry
 
Thermal PropertiesOriginal ValueComments
Oxygen Index 50 - 60 %
 
Descriptive Properties
Filament Count312000
Tow0.25-0.65%Tow Sizing
 61-67 gmTow Yield

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

ETEIJIN902 / 277912

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.