Description: AKROMID B3 GF 15 RM-M black (3440) is a 15% glass fiber reinforced, hydrolysis and chemical stabilized polyamide 6 with low humidity absorption and very good surface finish. Applications are housings and other dimensional stable parts in the automotive and electronic industry demanding high resistance against CaCl2 solvents, as well as a very good surface. Additive: Hydrolysis Resistant Features: - Good Chemical Resistance
- Good Surface Finish
- Low Moisture Absorption
- Good Dimensional Stability
- Hydrolysis Resistant
- Solvent Resistant
Uses:- Automotive Application
- Electrical/Electronic Applications
- Housings
Information provided by Akro-Plastic GmbH |