MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Denka MALECCA K-200 ABS
Categories: Polymer; Thermoplastic; ABS Polymer

Material Notes: A heat-resistant ABS resin based on "DENKA IP" – a Styrene-N-Phenylmaleimide copolymer. It has been designed as an easy-to-use resin by improving conventional heat-resistant ABS resins which had defects in terms of moldability, thermal stability, and impact resistance.

Applications

  • Mobile phones
  • vehicle-mounted audio equipment
  • automotive interior components
  • home electric appliances
  • OA equipment, etc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.06 g/ccASTM D792
Density 1.07 g/ccISO 1183
Melt Flow 6.0 g/10 min
@Load 10.0 kg,
Temperature 220 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 114ASTM D785
 114ISO 2039-2
Tensile Strength at Break 41.0 MPaASTM D638
 48.0 MPa50mm/min; ISO 527-2
Tensile Strength, Yield 39.0 MPaISO 527-2
Elongation at Break 28 %ISO 527-2
Tensile Modulus 2.50 GPa1mm/min; ISO 527-1
Flexural Strength 75.0 MPa15mm/min; ASTM D790
 78.0 MPaISO 178
Flexural Modulus 2.35 GPa15mm/min; ASTM D790
 2.45 GPa2mm/min; ISO 178
Izod Impact, Notched 196 J/m
@Temperature 23.0 °C
ASTM D256
Charpy Impact, Notched 1.90 J/cm²ISO 179-2
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °CISO 75-2
 106 °CASTM D648
Vicat Softening Point 115 °C50N; ISO 306
Flammability, UL94 HB

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Denka MALECCA K-100 ABS
Denka MALECCA K-096 ABS
Denka MALECCA K-090 ABS
Overview of materials for Nylon 66, Extruded
Overview of materials for AISI 4000 Series Steel

PDENK004 / 29668

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.