MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Total PPH 3571 Polypropylene, Film Extrusion Grade
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP); Polypropylene, Film Grade

Material Notes: Homopolymer film grade

Low Residuals - Fina 3571 utilizes the new Fina proprietary process technology to provide extremely low residuals for improved color stability and clarity.

Slip/Antiblock - Fina 3571 is available with custom slip and antiblock packages.

FDA - Fina 3571 complies with all applicable FDA regulations for food contact applications.

Recommended Applications - Fina 3571 is recommended for use in non-oriented cast film processes for manufacture of packaging films.

Processing - Fina 3571 resin processes on film extrusion equipment with typical melt temperatures of 450- 525°F (232-274°C)

Data provided by the manufacturer, Total Petrochemicals.

Total Petrochemicals acquired former Fina and Atofina plastics product lines.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.905 g/cc0.0327 lb/in³ASTM D1505
Water Vapor Transmission 11.0 g/m²/day
@Temperature 37.8 °C
0.708 g/100 in²/day
@Temperature 100 °F
90% RH; thickness not specified; ASTM E96
Melt Flow 9.0 g/10 min
@Temperature 230 °C
9.0 g/10 min
@Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 55.2 MPa8010 psiASTM D882
Film Elongation at Break, MD 500 %500 %Orientation not specified; ASTM D882
Secant Modulus 0.793 GPa115 ksiASTM D882
Dart Drop 0.780 g/micron19.8 g/milF50; ASTM D 1709
 
Thermal PropertiesMetricEnglishComments
Melting Point 163 °C325 °FDSC
 
Optical PropertiesMetricEnglishComments
Haze 2.0 %2.0 %ASTM D1003
Gloss 80 %80 %45°; ASTM D2457
 
Processing PropertiesMetricEnglishComments
Melt Temperature 232 - 274 °C450 - 525 °Ffilm extrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Nylon 6, Film Grade
Overview of materials for Thermoplastic Olefinic Elastomer (TPO), Film Grade
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced
Overview of materials for Medium Density Polyethylene (MDPE), Film Grade
Kinlead ML11 General Grade BOPP Matt Film (thickness: 30 µm)

PFIN21 / 38351

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.