MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Mitsubishi Novaduran® 5010G30 Polybutylene Terephthalate
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled

Material Notes: Standard. 30% GF reinforced UL-HB grade. Excellent mechanical properties. Excellent heat resistance. Excellent moldability and flowability. Low moisture absorption rate for high dimensional stability. Excellent surface gloss and color. Excellent oil and chemical resistance. Excellent electrical properties. Excellent friction and abrasion resistance. Flame retardant grades also available.

Information provided by Mitsubishi Engineering Plastics Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.53 g/ccISO 1183
Water Absorption 0.070 %
@Temperature 23.0 °C
Immersion
Linear Mold Shrinkage, Flow 0.0040 cm/cm
@Thickness 2.00 mm
100 mm long x 100 mm wide
Linear Mold Shrinkage, Transverse 0.012 cm/cm
@Thickness 2.00 mm
100 mm long x 100 mm wide
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 140 MPaISO 527-1,2
Elongation at Break 3.0 %ISO 527-1,2
Tensile Modulus 9500 MPaISO 527-1,2
Flexural Strength 215 MPaISO 178
Flexural Modulus 9000 MPaISO 178
Charpy Impact Unnotched 59.0 kJ/m²ISO 179-1
Charpy Impact, Notched 10.0 kJ/m²ISO 179-2
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 2.00e+16 ohm-cmIEC 60093
Surface Resistance 5.00e+16 ohmIEC 60093
Dielectric Constant 3.4
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 24.0 kV/mm
@Thickness 2.00 mm
IEC 60243-1
 27.0 kV/mm
@Thickness 1.00 mm
IEC 60243-1
Dissipation Factor 0.016
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 400 - 600 VUL746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 20.0 µm/m-°C
@Temperature -30.0 - 120 °C
ISO 11359-2
 20.0 µm/m-°C
@Temperature -30.0 - 50.0 °C
ISO 11359-2
 20.0 µm/m-°C
@Temperature 50.0 - 120 °C
ISO 11359-2
CTE, linear, Transverse to Flow 80.0 µm/m-°C
@Temperature -30.0 - 50.0 °C
ISO 11359-2
 110 µm/m-°C
@Temperature -30.0 - 120 °C
ISO 11359-2
 140 µm/m-°C
@Temperature 50.0 - 120 °C
ISO 11359-2
Melting Point 224 °CISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) <= 220 °CISO 75-1,2
Deflection Temperature at 1.8 MPa (264 psi) 207 °CISO 75-1,2
Flammability, UL94 HB
@Thickness 0.800 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Polyplastics Duranex® 3300 Polybutylene Terephthalate (PBT), Standard, 30% GF filled
Polyplastics Duranex® CRN7000 Polybutylene Terephthalate (PBT), Low gas generation, Low contact contamination, FR, UL approved regrind 50%
Celanese Celanex® 3300 PBT, 30% Glass Reinforced
Celanese Nilit Nilitop BT G6 General Purpose, 30% Glass Fiber Reinforced PBT
LATI Later 4 G/30 PBT, 30% Glass Fiber Reinforced

PMITSU9056 / 191729

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.