MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Westlake Plastics Lennite® GUR1050 (Type II) UHMW-PE For Medical Applications  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); UHMW PE (Ultra High Molecular Weight PE)

Material Notes: Replaced by Lennite WM .

Medical grade Lennite UHMWPE is produced from premium resins in accordance with ASTM specification F648 and International Standard ISO 5834-1 for surgical implants. Westlake Plastics' proprietary manufacturing processes and stringent quality control permit a well consolidated and consistent fabricated form. Recommended sterilization techniques include EtO gas, cold sterilization and limited gamma irradiation.

Applications Include:

  • Total hip and knee joint prosthesis
  • Various other surgical implants
  • Medical devices

Advantages of Medical Grade Lennite UHMWPE:

  • Lot controlled and traceable
  • ASTM F-648 and ISO 5834-1/2 Compliant
  • Stress relieved
  • Custom certifications available

Information provided by Westlake Plastics Company.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 0.934 g/ccResult
 0.927 - 0.944 g/ccRequirement
Ash 0.000055 %Result
 <= 0.00015 %Requirement
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break >= 27.0 MPaRequirement
 51.9 MPaResult
Tensile Strength, Yield >= 19.0 MPaRequirement
 22.7 MPaResult
Elongation at Break >= 300 %Requirement
 390 %Result
Izod Impact, Notched (ISO) >= 73.0 kJ/m²Requirement
 136 kJ/m²Result
Charpy Impact, Notched >= 90.0 kJ/m²Requirement
 149 kJ/m²Result

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Westlake Plastics Lennite® GUR1020 (Type I) UHMW-PE For Medical Applications
Westlake Plastics Lennite® Biocompatible Implant Grade UHMW-PE
LyondellBasell Plexar® PX2049 Extrudable Tie-Layer Resin - Anhydride Modified HDPE
Overview of materials for High Density Polyethylene (HDPE), Ultra High Molecular Weight
Polikim ULPOLEN® 1000 UHMWPE Standard

PWEST999 / 131209

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.