MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Teijin Panlite® G-3415R Glass Fiber Reinforced Polycarbonate Resin
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Glass Fiber Filled, Flame Retardant

Material Notes: GF 15% reinforced and mold release grade, meeting UL 94 V-2.

Applications:

  • Mechanical, electric and electronic components that need mechanical property e.g., stiffness
  • Precision machinery components that need dimensional accuracy.
  • Information provided by Teijin Chemicals Ltd.

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Density 1.30 g/cc0.0470 lb/in³ISO 1183
    Moisture Absorption 0.150 %
    @Temperature 23.0 °C,
    Time 86400 sec
    0.150 %
    @Temperature 73.4 °F,
    Time 24.0 hour
    ISO 62
    Linear Mold Shrinkage, Flow 0.0020 - 0.0040 cm/cm
    @Thickness 4.00 mm
    0.0020 - 0.0040 in/in
    @Thickness 0.157 in
    Teijin method
    Linear Mold Shrinkage, Transverse 0.0040 - 0.0060 cm/cm
    @Thickness 4.00 mm
    0.0040 - 0.0060 in/in
    @Thickness 0.157 in
    Teijin method
     
    Mechanical PropertiesMetricEnglishComments
    Tensile Strength at Break 85.0 MPa12300 psiISO 527-2/5
    Elongation at Break 3.0 %3.0 %ISO 527-2/5
    Tensile Modulus 5.00 GPa725 ksiISO 527-2/1
    Flexural Strength 130 MPa18900 psi2.0 mm/min; ISO 178
    Flexural Modulus 4.40 GPa638 ksi2.0 mm/min; ISO 178
    Charpy Impact Unnotched 5.00 J/cm²23.8 ft-lb/in²ISO 179
    Charpy Impact, Notched 1.00 J/cm²4.76 ft-lb/in²ISO 179
     
    Electrical PropertiesMetricEnglishComments
    Volume Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cmIEC 60093
    Surface Resistance >= 1.00e+15 ohm>= 1.00e+15 ohmIEC 60093
    Dielectric Constant  3.3
    @Frequency 100 Hz
    3.3
    @Frequency 100 Hz
    IEC 60250
     3.3
    @Frequency 1e+6 Hz
    3.3
    @Frequency 1e+6 Hz
    IEC 60250
    Dielectric Strength 35.0 kV/mm889 kV/inshort time test; IEC 60243-1
    Dissipation Factor  0.0010
    @Frequency 100 Hz
    0.0010
    @Frequency 100 Hz
    IEC 60250
     0.0090
    @Frequency 1e+6 Hz
    0.0090
    @Frequency 1e+6 Hz
    IEC 60250
     
    Thermal PropertiesMetricEnglishComments
    CTE, linear, Parallel to Flow 30.0 µm/m-°C16.7 µin/in-°FISO 11359-2
    CTE, linear, Transverse to Flow 60.0 µm/m-°C33.3 µin/in-°FISO 11359-2
    Deflection Temperature at 0.46 MPa (66 psi) 150 °C302 °Funannealed; ISO 75-2/B
    Deflection Temperature at 1.8 MPa (264 psi) 147 °C297 °Funannealed; ISO 75-2/A
    Vicat Softening Point 152 °C306 °FISO 306/B50
    UL RTI, Electrical 130 °C
    @Thickness 1.50 mm
    266 °F
    @Thickness 0.0591 in
    UL 746
    UL RTI, Mechanical with Impact 125 °C
    @Thickness 1.50 mm
    257 °F
    @Thickness 0.0591 in
    UL 746
    UL RTI, Mechanical without Impact 130 °C
    @Thickness 1.50 mm
    266 °F
    @Thickness 0.0591 in
    UL 746

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    Users viewing this material also viewed the following:
    Overview of materials for Polycarbonate, 10% Glass Filled
    Avient Edgetek® PC-30GF/000 FR BLACK Polycarbonate - 30% Glass Fiber Reinforced - Flame Retardant
    Overview of materials for Polycarbonate, 20% Glass Filled
    Overview of materials for Polycarbonate, Carbon Fiber Reinforced
    Overview of materials for Polycarbonate, Foam Grade, Glass Filled

    PTEIJ24 / 69713

    Aluminum Castings

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.