MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Sandvik 13C26 razor blade steel Strip
Categories: Metal; Ferrous Metal; Martensitic

Material Notes: Sandvik 13C26 is a martensitic stainless chromium steel characterized by:
  • Excellent metallurgical properties
  • Close tolerances
  • Smooth surface, extra accuracy on flatness and straightness
  • Good blanking properties
  • Good hardening properties
  • Good grinding and honing properties, facilitating the manufacture of high quality edges
  • Good corrosion resistance (hardened and tempered condition)
  • Consistent material properties from coil to coil, from delivery to delivery

Information provided by Sandvik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.70 g/cc
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.68 %
Manganese, Mn 0.70 %
Phosphorus, P <= 0.025 %
Silicon, Si 0.40 %
Sulfur, S <= 0.010 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3RE60 Duplex Stainless Steel, Annealed Pipe, UNS S31500
ATI Allegheny Ludlum AL 2003â„¢ Duplex Stainless Steel
AK Steel NITRONIC® 19-D Duplex Stainless Steel
Titanium Ti-16V-2.5Al, Duplex Annealed
Uranus 50 Duplex Stainless Steel, UNS S32404 (Composition Spec)

NSANDV5070 / 199634

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.