MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
3M Scotchkote™ LW 405 Epoxy Concrete Mortar
Categories: Polymer; Thermoset; Epoxy

Material Notes: Scotchkote Epoxy Concrete Mortar LW 405 has been specifically developed as a three component 100% solids light weight repair mortar for use on concrete surfaces.

Product Features:

  • Designed for application by trowel or float
  • Can be used to form wall/floor covings
  • Excellent hold up on vertical and overhead surfaces
  • High abrasion resistance and excellent adhesion
  • Unaffected by most industrial chemicals

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 100 %
Volatile Organic Compounds (VOC) Content 0.00 g/l
pH 10
Thickness 236 mil
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 80
Compressive Strength 6000 psiASTM D695
 
Processing PropertiesOriginal ValueComments
Cure Time 8.00 hourHard Dry
 24.0 hourFull Hardness
 168 hourFull Cure
 
Descriptive Properties
AppearanceLight Gray

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Coastal Enterprises Plus™ PBHT-15 High Density Urethane Foam
Alliance Polymers Zythane™ 3045D Thermoplastic Polyurethane Elastomer
Covestro Desmopan® 588 Thermoplastic Polyurethane
Northstar Polymers MPP-A47A Liquid Castable Polyurethane
Overview of materials for Thermoset Polyurethane, Liquid

PMM35320 / 170067

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.