MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polynt POLYCOR® TOPCOAT ISO BR
Categories: Polymer; Thermoset

Material Notes: A pre-accelerated top coat based on Isophthalic unsaturated polyester resin. It is cured using MEKP peroxide.

Appearance: Product is available in clear, white, off-white and wide range of colors and can be color matched according to a particular demand. The product is formulated to assure a hide in wet film thickness of 500µm. However some bright shades may have a hide slightly lower opacity. TOP COAT : Contains wax.

Properties / Advantages: Specially formulated for finishing applications. The product is easy to use with highly controlled rheological properties providing high resistance to sagging. This product has good resistance to yellowing over time. It has good gloss retention properties. This product has good water resistance properties. Top coats are not intended for constant water immersion applications. This product has resilient mechanical properties.

Application: This top coat is ready to use by application with a brush. Mix the product slowly but thoroughly for 10 minutes prior to each shift start up. Apply the correct film thickness. A wet film thickness between 300 to 600µm is required ideally working with a brush to ensure a level even thickness of 500 micron Check that the correct level of MEKP is added. A level of 1,8% is recommended. Do not use more than 3% or lower than 1,2% MEKP catalyst. Minimum application temperature : 15°C This product is not designed for use with a spray gun.

Use Areas: This TOP COAT product is formulated to be applied to the back surface of laminates to provide a tack free surface finish. It should not be used as a gel coat. This topcoat is formulated to meet the rigid requirements of transportation, boating and sanitary applications.

Information provided by Polynt Composites.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 - 1.26 g/cc0.0379 - 0.0455 lb/in³
Solids Content 64 - 71 %64 - 71 %15mn at 150°C
Viscosity 21000 - 26000 cP21000 - 26000 cPSpindle 5 - 5 rpm
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 59.0 MPa8560 psiISO 527
Elongation at Break 3.8 %3.8 %ISO 527
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 54.0 °C129 °FNFT ISO 75
 
Processing PropertiesMetricEnglishComments
Cure Time  15.0 - 25.0 min
@Temperature 25.0 °C
0.250 - 0.417 hour
@Temperature 77.0 °F
Peak time; 200g - 25°C - 1,8% MEKP
 45.0 - 80.0 min
@Temperature 20.0 °C
0.750 - 1.33 hour
@Temperature 68.0 °F
Film cure; 500µ - 20°C - 2% MEKP
Gel Time 8.00 - 13.0 min
@Temperature 25.0 °C
8.00 - 13.0 min
@Temperature 77.0 °F
200g - 25°C - 1,8% MEKP
Shelf Life 4.00 Month4.00 Month
 
Descriptive Properties
Peak Exotherm160-190°C200g - 25°C - 1,8% MEKP
Sag Resistance500 µmwet
Thixotropic Index3.8-4.45/50 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPOLYN9254 / 231849

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.