MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Ineos H02C-00 Polypropylene Homopolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Blow Molding Grade; Polypropylene, Extrusion Grade; Polypropylene, Sheet/Thermoforming Grade

Material Notes: This is a low flow rate, high clarity homopolymer designed for extrusion, thermoforming, blow molding, and rigid packaging. Applications that require good see-through clarity combined with good heat resistance can benefit from this grade of material. This material meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520.

    Applications
  • Thermoformed packaging (cups, containers, lidding)
  • Extrusion blow molded containers and bottles
  • Injection blown molded containers and bottles
  • Extruded sheet and profiles

    Benefits
  • Excellent clarity
  • Excellent processability

Information provided by Ineos Olefins & Polymers USA

Key Words: Low flow rate, high clarity
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.911 g/ccASTM D792
Melt Flow 2.3 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 99Injection Molded; ASTM D785
Tensile Strength at Break 2600 psi2.0 in/min, Injection Molded; ASTM D638
Tensile Strength, Yield 5300 psi2.0 in/min, Injection Molded; ASTM D638
Elongation at Break 120 %2.0 in/min, Injection Molded; ASTM D638
Elongation at Yield 9.1 %2.0 in/min, Injection Molded; ASTM D638
Flexural Modulus, 1% Secant 240000 psiInjection Molded; ASTM D790A
Izod Impact, Notched 0.500 ft-lb/inInjection Molded; ASTM D256
Izod Impact, Notched (ISO) 1.33 ft-lb/in²Area, Injection Molded; ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 230 °FUnannealed, Injection Molded; ASTM D648
Vicat Softening Point 309 °FASTM D1525
 
Optical PropertiesOriginal ValueComments
Haze 30 %
@Thickness 1.27 mm
ASTM D1003
Gloss 96 %60°; ASTM D2457
Transmission, Visible 26 %
@Thickness 1.27 mm
plaque, Diffuse Transmittance; ASTM D1003
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.
 
Descriptive Properties
ProcessBlow Molding
 Extrusion
 Sheet Extrusion
 Thermoforming

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Avient Maxxam™ FR PP 301 S Polypropylene
LyondellBasell Petrothene® LM600731X01 High Density Polyethylene, Sheet Extrusion Grade
Ineos H02C-01 Polypropylene Homopolymer
Celanese Celcon® M50 POM, Unfilled
Celanese Celstran® PP-GF30-03 Natural PP, 30% Glass Reinforced

PINEOS017 / 99338

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.