MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Refractory Metals

Mi-Tech Metals CW75 75 Tungsten/25 Copper PM Metal Composite
Categories: Metal; Metal Matrix Composite; Nonferrous Metal; Refractory Metal; Tungsten Alloy

Material Notes: RWMA Class 11.

Mi-Tech refractory alloys are manufactured by pressing, sintering, and infiltrating tungsten with copper or silver.

Typical Resistance Welding Applications: Class 11 Cu-W (a harder material than Class 10) is used for facings and inserts for flash and butt welding dies, projection welding electrodes, seam welding bearing inserts, facings for electro-forming and electro-forging dies. Often used for EDM electrodes for greater wear ratios.

Mi-Tech Copper-Tungsten and Silver-Tungsten are manufactured as electrode materials for EDM (Electrical Discharge Machining), ECM (Electro Chemical Machining) and ECD (Electro Chemical Deburring).

Mi-Tech materials are also manufactured by the powder metallurgy techniques of pressing, sintering and infiltrating tungsten with copper or silver. This assures a high performance electrode providing greater cutting stability, excellent machinability and reduced down time. For extremely close tolerance work, this product holds dimensions and will not break down due to porosity and other structural deficiencies sometimes found in other Copper-Tungsten electrode alloys.

Mi-Tech Copper-Tungsten is well suited for machining carbide dies. Further more, it offers greater cutting stability in machining refractory metals and exotics.

Tungsten alloys used for EDM and ECM applications are far superior when fine surface finishes, deep narrow slots or ribs and small precise holes are required. Tungsten alloys are preferred when matching extremely detailed sections. In the ECM process, Copper-Tungsten withstands erosive effects of short circuit malfunctions far better than other materials.

Data provided by Mi-Tech Metals.

Key Words: Powder Metallurgy Metal Composite Tungsten Alloy RWMA Class 11
Vendors: Eagle Alloys Corporation is a leading supplier of quality metals and alloys. Our staff prides itself on working fast, efficiently and courteously to get you the information you need. Call (800) 237-9012 or visit www.EagleAlloys.com.

PLANSEE SE: Whether it's high temperatures, aggressive chemicals or extreme mechanical loading: PLANSEE supplies a suitable product solution in refractory metals or composite materials. As the world market leader in powder metallurgically produced high performance materials we combine outstanding materials knowledge with profound applications and technology know-how. Visit us at www.plansee.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density >= 14.5 g/cc>= 0.524 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 9090
Tensile Strength, Ultimate 621 MPa90100 psi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000370 ohm-cm0.00000370 ohm-cm
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 25 %25 %
Tungsten, W 75 %75 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
H.C. Starck Amperit® 525.2 Sintered Tungsten Carbide - Cobalt (WC-Co) 83-17
Lucas-Milhaupt Silvaloy® 505 Carbide Brazing Alloy
Phosphorus deoxidized tellurium bearing Copper, UNS C14500, H04 Temper 13 mm and 25 mm rods
Tungsten Carbide, WC
Wingate Alloys Dyconite Tungsten Carbide Overlay Plate

NMITECH11 / 18421

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.