MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Akro-Plastic Akromid® C3 GF 30 5 XTC (4499) PA66/6 Dry, 30% Glass Filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6/66; Nylon 66/6, 30% Glass Fiber Reinforced

Material Notes: AKROMID® B (Polyamide 6.6/6 Blend) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatures as well as easy processing. AKROMID® C is an engineering plastic compound that allows a broad range of possible applications. On the basis of these standard types, we are able to develop individual compounds for special application needs.

Information provided by Akro-Plastic GmbH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.39 g/ccISO 1183
Filler Content 30 %ISO 1172
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 190 MPa5 [mm/min]; ISO 527-1/2
Tensile Stress at Strain 28.5 MPa
@Strain 1 %,
Temperature 220 °C
 38.0 MPa
@Strain 3 %,
Temperature 220 °C
 47.5 MPa
@Strain 1 %,
Temperature 150 °C
 47.5 MPa
@Strain 2 %,
Temperature 220 °C
 95.0 MPa
@Strain 6.0 %,
Temperature 150 °C
 114 MPa
@Strain 3 %,
Temperature 150 °C
 142.5 MPa
@Strain 5.0 %,
Temperature 23.0 °C
 285 kg(f)/cm²
@Strain 1 %,
Temperature 23.0 °C
 361 MPa
@Strain 3 %,
Temperature 23.0 °C
Elongation at Break 3.7 %5 [mm/min]; ISO 527-1/2
 2.5 %
@Treatment Temp. 210 °C,
Time 1.80e+7 sec
 2.5 %
@Treatment Temp. 230 °C,
Time 1.08e+7 sec
 2.7 %
@Treatment Temp. 210 °C,
Time 1.08e+7 sec
 2.8 %
@Treatment Temp. 230 °C,
Time 7.20e+6 sec
 3.0 %
@Treatment Temp. 210 °C,
Time 1.80e+6 sec
 3.0 %
@Treatment Temp. 230 °C,
Time 1.80e+6 sec
Tensile Modulus 9900 MPa1 [mm/min]; ISO 527-1/2
Charpy Impact Unnotched 95.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched 13.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+12 ohm-cmIEC 60093
Surface Resistance 1.00e+13 ohmIEC 60093
Comparative Tracking Index 600 VSolution A; IEC 60112
 
Thermal PropertiesOriginal ValueComments
Melting Point 255 °CDIN EN 11357-1/3
Deflection Temperature at 0.46 MPa (66 psi) 250 °CHDT/B; ISO 75-2
Deflection Temperature at 1.8 MPa (264 psi) 230 °CHDT/A; ISO 75-2
Flammability, UL94 HB
@Thickness 1.60 mm
 
Processing PropertiesOriginal ValueComments
Feed Temperature 60.0 - 80.0 °C
Nozzle Temperature 280 - 295 °C
Zone 1 225 - 300 °C
Zone 2 225 - 300 °C
Zone 3 225 - 300 °C
Zone 4 225 - 300 °C
Melt Temperature 280 - 310 °C
Mold Temperature 80.0 - 100 °C
Drying Temperature 80.0 °C
Dry Time 2.00 hour
Hold Pressure 30.0 - 80.0 MPa
Back Pressure 5.00 - 10.0 MPa
 
Descriptive Properties
Rate acc. FMVSS 302,(<100/min)Passed>1 [mm] Thickness
Resistance to AcetaldehydeFail40% Conc. at 23°C
Resistance to Acetic AcidPass20% Conc. at 23°C
Resistance to AcetonePass100% Conc. at 23°C
Resistance to AcetonitrilePass100% Conc. at 23°C
Resistance to AcrylonitrilePass100% Conc. at 23°C
Resistance to Allyl alcoholFail96% Conc. at 23°C
Resistance to Amyl alcoholPass100% Conc. at 23°C
Resistance to Aqueous AmmoniaPass10% Conc. at 23°C
Resistance to BenzeneFail100% Conc. at 40°C
 Pass100% Conc. at 23°C
Resistance to BiodieselPass100% Conc. at 23°C
Resistance to Boric acidFail100% Conc. at 23°C
 Pass10% Conc. at 23°C
Resistance to Brake fluid (DOT 4)Fail100% Conc. at 130°C
 Pass100% Conc. at 23°C
Resistance to Calcium chloride, alcoholicFail10% Conc. at 23°C
Resistance to Calcium chloride, aqueousPass10% Conc. at 23°C
Resistance to Carbonic acidPass100% Conc. at 60°C
Resistance to Caustic potash solution, aqueousPass50% Conc. at 23°C
Resistance to ChlorineFail100% Conc. at 23°C
Resistance to Chlorine waterFail100% Conc. at 23°C
Resistance to Chloroacetic acidFail50% Conc. at 23°C
Resistance to Chromic acidFail10% Conc. at 23°C
Resistance to CyclohexanePass100% Conc. at 23°C
Resistance to CyclohexanolPass100% Conc. at 23°C
Resistance to Dichloro-Acetic acidFail50% Conc. at 23°C
Resistance to Diesel fuel (DIN 51601)Pass100% Conc. at 23°C
Resistance to EthanolPass96% Conc. at 23°C
Resistance to Ethylene glycol/waterFail50% Conc. at 120°C
Resistance to Formaldehyde, aqueousPass10% Conc. at 23°C
Resistance to Formic acidFail2% Conc. at 23°C
Resistance to GlycerinPass100% Conc. at 23°C
Resistance to Hydraulic oil H and HL (DIN 51524)Pass100% Conc. at 100°C
Resistance to Hydrogen chloride, gasFail100% Conc. at 23°C
Resistance to Iso-octanolPass100% Conc. at 23°C
Resistance to IsopropanolPass100% Conc. at 23°C
Resistance to MethanolPass100% Conc. at 23°C
Resistance to Methylene chlorideFail100% Conc. at 23°C
Resistance to Motor oil (SAE 10W-40)Pass100% Conc. at 130°C
 Pass100% Conc. at 23°C
Resistance to Natural GasPass100% Conc. at 23°C
Resistance to Nitric acidFail40% Conc. at 23°C
Resistance to Oleic acidPass100% Conc. at 23°C
Resistance to OzoneFail100% Conc. at 23°C
Resistance to PhenolFail100% Conc. at 23°C
Resistance to Phosphoric acidFail30% Conc. at 23°C
Resistance to Potassium chloride, aqueousPass10% Conc. at 23°C
Resistance to Potassium permanganate, aqueousFail10% Conc. at 23°C
Resistance to Sodium chloride, aqueousPass10% Conc. at 23°C
Resistance to Sodium hydroxide solution, aqueousPass1% Conc. at 23°C
Resistance to Sodium hypochlorite, aqueousFail10% Conc. at 23°C
Resistance to Transmission oil (ATF m 1375.4)Pass100% Conc. at 150°C
Resistance to Urea, aqueousPass20% Conc. at 23°C
Resistant to Carbon disulfidePass100% Conc. at 23°C
Resistant to Carbon tetrachloridePass100% Conc. at 23°C
Resistant to Citric acidPass10% Conc. at 23°C
Resistant to Ethyl acetatePass100% Conc. at 23°C
Resistant to Hydrochloric acidFail36% Conc. at 23°C
Resistant to Hydrogen peroxideFail23°C
Resistant to SeawaterPass100% Conc. at 23°C
Resistant to Silicone fluidPass23°C
Resistant to Sodium hypochlorite, aqueousFail5% Conc. at 23°C
Resistant to Sulfuric acidFail10% Conc. at 23°C
 Fail96% Conc. at 23°C
Resistant to Super-grade petrol (DIN 51600)Pass100% Conc. at 23°C
Resistant to ToluolPass100% Conc. at 23°C
Resistant to WaterPass100% Conc. up to 50°C
Resistant to XylolPass100% Conc. at 23°C
Resistant to Zinc chloride, aqueousFail50% Conc. at 23°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Akro-Plastic Akromid® B3 GF 30 S1 (2091) PA66/6 Dry, 30% Glass Filled
Akro-Plastic Akromid® C3 GF 30 5 XTC (4499) PA66/6 Conditioned, 30% Glass Filled
Overview of materials for Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled
Akro-Plastic Akromid® B3 GF 30 S1 (2091) PA66/6 Conditioned, 30% Glass Filled
Mitsubishi Chemical Advanced Materials Nylatron™ GS PA66 with MoS2, extruded

PAKRO125 / 182712

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.