Availability: North America Forms: Pellets Filler/Reinforcement: Glass Fiber, 40% Filler by Weight Additive: Heat Stabilizer and Molybdenum Disulfide Lubricant(2%) Features: Lubricated and Heat Stabilized Appearance: Natural Color Information provided by TP Composites, Inc. |