Catalyst CT/7-LR UV LB is a polyolefin based masterbatch to be used with cable silane crosslinkable compounds in the amount suggested for each material. It is designed to minimize the blooming effect that could occur in warm areas. Developed for Polidan®, Polidiemme® and Cogegum® GFR series compounds, it is suitable for most severe long term ageing conditions. It has a low catalytic activity and it confers improved UV/VIS and aging resistance. Catalyst CT/7-LR UV LB can be used in a wide application range due to its catalytic activity and the anti-ageing effect given to the final product. It contains also a metal deactivator that allows its use also in direct contact with untinned copper. Availability: Features:- Copper Contact Stabilized
- Halogen Free
Uses:- Wire & Cable Applications
Information provided by Solvay |