MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Eastman Tacolyn™ 5003 Resin Dispersion
Categories: Polymer

Material Notes: Product Description: Tacolyn™ 5003 resin dispersion is an aqueous, 45% solids, solvent-free, anionic hydrocarbon resin dispersion. It is recommended as a single tackifier for anionic polychloroprene latex polymers used in contact adhesive applications. When used as a modifier for contact adhesives, Tacolyn™ 5003 imparts outstanding high temperature performance, excellent contactability and good moisture resistance without the use of a second reinforcing tackifier.

Application/Uses:

  • Building and Construction
  • Contact Adhesives
  • Pressure sensitive adhesives
  • Tapes and Labels
  • Waterborne Adhesives
Key Attributes:
  • APE-free
  • Good moisture resistance
  • Good thermal and UV stability
  • Promotes cohesion
  • Promotes high temperature performance

Information provided by Eastman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.02 g/cc
Solids Content 45 %
Particle Size >= 250 µm
pH >= 7.0Tolerance Rang
 11
Brookfield Viscosity 1000 cP
 
Thermal PropertiesOriginal ValueComments
Ring & Ball Softening Point 130 °CASTM E 28

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEATM5601 / 222795

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.