MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Corning Astra™ Alkaline Earth Boro-Aluminosilicate Display Glass
Categories: Ceramic; Glass; Optical

Material Notes: Astra™ Glass features a blend of low total pitch variation, low total thickness variation, and low sag to enable high-performance tablets and notebooks, as well as the next generation of 8K LCD and OLED TVs. With an optimum blend of attributes and attractive panel economics, Astra Glass performs well in oxide thin-film transistor (TFT) backplane manufacturing processes. It is available as a fusion drawn sheet.

Information provided by Corning Incorporated.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.52 g/cc0.0910 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 651651kg(f)/mm² (200 g load; 25 s dwell)
Modulus of Elasticity 81.0 GPa11700 ksi
Poissons Ratio 0.230.23
Shear Modulus 33.0 GPa4790 ksi
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity  5.00e+9 ohm-cm
@Temperature 500 °C
5.00e+9 ohm-cm
@Temperature 932 °F
 1.30e+14 ohm-cm
@Temperature 250 °C
1.30e+14 ohm-cm
@Temperature 482 °F
 1.60e+25 ohm-cm
@Temperature 25.0 °C
1.60e+25 ohm-cm
@Temperature 77.0 °F
Dielectric Constant 5.8
@Frequency 1000 Hz,
Temperature 20.0 °C
5.8
@Frequency 1000 Hz,
Temperature 68.0 °F
Dissipation Factor 0.0020
@Frequency 1000 Hz,
Temperature 20.0 °C
0.0020
@Frequency 1000 Hz,
Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear 3.30 µm/m-°C
@Temperature 0.000 - 300 °C
1.83 µin/in-°F
@Temperature 32.0 - 572 °F
Specific Heat Capacity  0.7703 J/g-°C
@Temperature 100 °C
0.1841 BTU/lb-°F
@Temperature 212 °F
 0.9069 J/g-°C
@Temperature 200 °C
0.2168 BTU/lb-°F
@Temperature 392 °F
 0.9492 J/g-°C
@Temperature 300 °C
0.2269 BTU/lb-°F
@Temperature 572 °F
 1.0169 J/g-°C
@Temperature 400 °C
0.24305 BTU/lb-°F
@Temperature 752 °F
 1.0666 J/g-°C
@Temperature 500 °C
0.25492 BTU/lb-°F
@Temperature 932 °F
Thermal Conductivity  1.128 W/m-K
@Temperature 100 °C
7.828 BTU-in/hr-ft²-°F
@Temperature 212 °F
 1.285 W/m-K
@Temperature 200 °C
8.918 BTU-in/hr-ft²-°F
@Temperature 392 °F
 1.303 W/m-K
@Temperature 300 °C
9.043 BTU-in/hr-ft²-°F
@Temperature 572 °F
 1.402 W/m-K
@Temperature 400 °C
9.730 BTU-in/hr-ft²-°F
@Temperature 752 °F
 1.446 W/m-K
@Temperature 500 °C
10.04 BTU-in/hr-ft²-°F
@Temperature 932 °F
Softening Point 1010 °C1860 °F107.6 Poise
Annealing Point 778 °C1430 °F1013 Poise
Strain Point 725 °C1340 °F1014.5 Poise
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.522
@Wavelength 589.3 nm
1.522
@Wavelength 589.3 nm
Abbe Number 62.4962.49
Transmission, Visible >= 90 %
@Wavelength 400 - 800 nm,
Thickness 0.400 mm
>= 90 %
@Wavelength 400 - 800 nm,
Thickness 0.0157 in
 
Descriptive Properties
Birefringence Constant292 (nm/cm)/(kg/mm²)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

CCORNG991x / 281580

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.