MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil Vistamaxx™ 8380 Performance Polymer
Categories: Other Engineering Material

Material Notes: Vistamaxx performance polymers have attributes such as: Transparency, Elasticity, Adhesion, Toughness, Filler loading, Cling/tackiness, Softness, Flexibility, Sealability.

Vistamaxx 8380 is primarily composed of isotactic propylene repeat units with random ethylene distribution, and is produced using ExxonMobil's proprietary metallocene catalyst technology. It has a low viscosity that enables its use in hot melt adhesives and as a process aid or viscosity modifier in extrusion and injection molding applications providing enhanced flow characteristics that can lead to efficiency and cycle time improvements.  

Availability:  Africa & Middle East, Europe, North America, Asia Pacific, Latin America.  Applications: Hot melt adhesives, polymer modification..  Uses: adhesives, compounding. Form:  pellets. Processing Method:  compounding, extrusion, injection molding.

Information provided by ExxonMobil.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.864 g/ccExxonMobil Method
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore C 18ASTM D 2240
 
Thermal PropertiesOriginal ValueComments
Melting Point 212 °FExxonMobil Method
Glass Transition Temp, Tg -24.0 °FExxonMobil Method
 
Descriptive Properties
Ethylene Content (%wt)12ExxonMobil Method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Alliance Polymers Viprene™ P70A-22U-BLK Thermoplastic Vulcanizate Elastomer
Alliance Polymers Viprene™ P60A-22U-NAT Thermoplastic Vulcanizate Elastomer
Alliance Polymers Viprene™ P60A-22U-BLK Thermoplastic Vulcanizate Elastomer
ExxonMobil Vistamaxx™ 6102 Propylene-based Elastomer
ExxonMobil Vistamaxx™ 8880 Performance Polymer

PEX98964 / 238345

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.