MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Covestro Desmodur® IL BA Polyurethane
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: Aromatic polyisocyanate based on toluene diisocyanate. As the hardener component for fast-drying two-component polyurethane coatings.

Properties / Applications: When combined with, for example, Desmophen® 1300, Desmodur® IL BA yields very fast-drying systems. These are used in, for example, the furniture industry where very short drying times and early sandability are required.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.10 g/ccDIN EN ISO 2811-3
Volatiles 47 - 51 %0.2 g / 120 °C / 100 °C; M020-ISO 3251
Viscosity 1600 - 2400 cPM014- ISO 3219/A.3
 
Thermal PropertiesOriginal ValueComments
Flash Point 25.0 °CDIN EN ISO 1523
 
Descriptive Properties
Color<2Iodine, M017-EN 1557
Content<0.5%Monomeric, M106-ISO 10283
 7.8-8.2%NCO, M105-ISO 11909

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro Desmodur® L 67 BA Polyurethane
Covestro Desmodur® I Polyurethane
Covestro Desmodur® HL BA Polyurethane
Covestro Desmodur® H Polyurethane
Covestro Desmodur® IL 1351 51% BA Polyurethane

PCOVEST0356 / 202139

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.