MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Titanium Grade 3, Annealed
Categories: Metal; Nonferrous Metal; Titanium Alloy; Unalloyed/Modified Titanium

Material Notes: Information provided by Allvac and the references.

Applications: Airframe skin, heat exchangers, cryogenic vessels, components for CPI equipment, condenser tubing, exhaust pipe shrouds. Sample was annealed 2 hr at 700°C.

Forms typically available: billet, bar, plate, sheet, strip, rod, wire, extrusions, tubing.

Titanium Grades 1,2,3,4,7,11,and 12 are all considered unalloyed and have similar mechanical properties.

Key Words: ASTM Grade 3; UNS R50550, CP titanium, C.P. titanium alloy
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 4.50 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 225
Hardness, Knoop 289Estimated from Rockwell C.
Hardness, Rockwell C 26
Hardness, Vickers 280Estimated from Rockwell C.
Tensile Strength 234 MPa
@Temperature 316 °C
Tensile Strength, Ultimate 520 MPa
Tensile Strength, Yield 450 MPa
Elongation at Break 25 %
Creep Strength 103 MPa
@Temperature 316 °C,
Time >=3.60e+6 sec
strain 3%
Rupture Strength >= 172 MPa
@Temperature 316 °C,
Time 3.60e+6 sec
Tensile Modulus 104 GPa
Modulus of Rigidity 38.6 GPa
Compressive Modulus 114 GPa
Notched Tensile Strength 790 MPaKt (stress concentration factor) = 3.0
Ultimate Bearing Strength 920 MPa
Bearing Yield Strength 650 MPa
Poissons Ratio 0.34
Fatigue Strength 250 MPa
@# of Cycles 1.00e+7
Kt (stress concentration factor) = 2.7
 280 MPa
@# of Cycles 1.00e+7
 290 MPa
@# of Cycles 1.00e+6
 295 MPa
@# of Cycles 100000
 340 MPa
@# of Cycles 10000
 340 MPa
@# of Cycles 1.00e+7
unnotched
Shear Modulus 39.0 GPa
Charpy Impact 27.0 JV-notch
Bend Radius, Minimum 2.5 t
@Thickness >=1.80 mm
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000540 ohm-cm
 0.0000900 ohm-cm
@Temperature 250 °C
 0.000120 ohm-cm
@Temperature 500 °C
 0.000150 ohm-cm
@Temperature 750 °C
 
Thermal PropertiesOriginal ValueComments
Heat of Fusion 325 J/gHigh Purity Ti.
CTE, linear 8.60 µm/m-°C
@Temperature 20.0 - 93.0 °C
 9.20 µm/m-°C
@Temperature 200 °C
 19.9 µm/m-°C
@Temperature 20.0 °C
perpendicular
Specific Heat Capacity 0.523 J/g-°C
 0.560 J/g-°C
@Temperature 200 °C
 0.620 J/g-°C
@Temperature 400 °C
 0.690 J/g-°C
@Temperature 600 °C
Thermal Conductivity 16.4 W/m-K
 18.1 W/m-K
@Temperature 200 °C
 18.1 W/m-K
@Temperature 400 °C
 19.1 W/m-K
@Temperature 600 °C
 21.5 W/m-K
@Temperature 800 °C
Melting Point <= 1660 °C
Liquidus 1660 °C
Beta Transus 920 °C
 
Optical PropertiesOriginal ValueComments
Emissivity (0-1) 0.30
@Temperature 710 °C
High purity Ti
Reflection Coefficient, Visible (0-1) 0.56High purity Ti; visible light.
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.10 %
Hydrogen, H <= 0.015 %
Iron, Fe <= 0.30 %
Nitrogen, N <= 0.050 %
Other, total <= 0.30 %
Oxygen, O <= 0.35 %
Titanium, Ti 99.1 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Titanium Grade 2, Annealed
Titanium Ti-6Al-4V (Grade 5), Annealed
Aluminum 6061-T6; 6061-T651
ATI Wah Chang Nb/Nb Alloy C-103
304 Stainless Steel (UNS S30400); Annealed Sheet

MTU031 / 14262

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.