MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Arkema Kynar Flex® LBG PVDF
Material Notes:

Information provided by Arkema.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.78 g/cc1.78 g/ccASTM D792
Density 1.78 g/cc0.0643 lb/in³ISO 1183
Water Absorption 0.030 %0.030 %Dry; Sim. to ISO 62
Viscosity 3.40e+6 - 3.80e+6 cP
@Shear Rate 100 1/s,
Temperature 230 °C
3.40e+6 - 3.80e+6 cP
@Shear Rate 100 1/s,
Temperature 446 °F
Melt; ASTM D3835
Melt Flow  3.2 g/10 min
@Load 21.6 kg,
Temperature 232 °C
3.2 g/10 min
@Load 47.6 lb,
Temperature 450 °F
cm³/10 min Volumetric Rate; ISO 1133
 3.0 - 8.0 g/10 min
@Load 21.6 kg,
Temperature 230 °C
3.0 - 8.0 g/10 min
@Load 47.6 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 35.0 MPa5080 psiASTM D638
 35.0 MPa5080 psiDry; ISO 527-1/-2
Elongation at Break >= 50 %>= 50 %Dry; ISO 527-1/-2
 <= 400 %<= 400 %ASTM D638
Elongation at Yield 10 %10 %Dry; ISO 527-1/-2
Flexural Modulus 1.03 GPa149 ksiASTM D790
Charpy Impact, Notched NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
Dry; ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 151 - 157 °C304 - 315 °FASTM D3418
 154 °C309 °F10°C/min; Dry; ISO 11357-1/-3
 
Descriptive Properties
Form as DeliveredPowder
Moisture SensitiveNo

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Arkema Kynar Flex® PPA 2200 PVDF
Arkema Kynar Flex® Ultraflex B PVDF
Arkema Kynar Superflex® 2500-20 PVDF
Arkema Kynar Flex® PPA 5300 PVDF
Arkema KYNAR FLEX® 3120-50 Polyvinylidene Fluoride Copolymer - Extrusion & Molding

PARKF720 / 193522

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.