MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Röchling Glastic Laminates/Shapes Polyester, Channels and Structural Shapes (GPO3)
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Polyester, TS; Thermoset Polyester Glass Filled BMC

Material Notes: Data provided by Glastic Corporation.

NEMA GPO-3. Average data - may vary with the size and shape of the electrical insulating structural product.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.80 g/ccASTM D792
Water Absorption 0.30 %ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Hardness, Barcol 50ASTM D2583
Tensile Strength, Ultimate 103 MPaASTM D638
Tensile Modulus 12.0 GPaASTM D638
Flexural Strength 172 MPaASTM D790
Flexural Modulus 8.00 GPaASTM D790
Compressive Strength 140 MPaEdgewise; ASTM D695
 290 MPaFlatwise; ASTM D695
Shear Strength 100 MPaASTM D732
Izod Impact, Notched 5.10 J/cmASTM D256
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 8.00 kV/mmPerpendicular, Short-term, in air; ASTM D149
Arc Resistance 185 secASTM D495
 
Thermal PropertiesOriginal ValueComments
CTE, linear 20.0 µm/m-°C
@Temperature 20.0 °C
ASTM D696
Thermal Conductivity 0.270 W/m-KASTM C177
UL RTI, Electrical 130 °CUL 746B
UL RTI, Mechanical with Impact 160 °CUL 746B
Flammability, UL94 V-0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
5754-H22 Aluminum
304 Stainless Steel
MarkeTech Silica Aerogel
Plenco 08122 Polyester BMC, Compression Molded
AISI 1045 Steel, Quenched and Tempered to 390 HB

PGLASL / 41922

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.