Almaak Anjacom® PC/ABS 050/45K PC/ABS
Categories:
Polymer
;
Thermoplastic
;
ABS Polymer
;
Polycarbonate/ABS Alloy, Unreinforced
Material Notes:
unreinforced, easy flowing, high impact modified, cold impact strength, natural color
Information provided by Almaak International GmbH.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.09
g/cc
0.0394
lb/in³
ISO 1183
Water Absorption
0.70 %
0.70 %
ISO 62
Moisture Absorption
0.200 %
0.200 %
50% RH; ISO 62
Linear Mold Shrinkage, Flow
0.0040
-
0.0060
cm/cm
0.0040
-
0.0060
in/in
ISO 294-4
Linear Mold Shrinkage, Transverse
0.0040
-
0.0080
cm/cm
0.0040
-
0.0080
in/in
ISO 294-4
Melt Flow
17
g/10 min
@Load 5.00 kg,
Temperature 260 °C
17
g/10 min
@Load 11.0 lb,
Temperature 500 °F
ISO 1133
Mechanical Properties
Metric
English
Comments
Tensile Strength, Yield
55.0
MPa
7980
psi
50 mm/min; ISO 527-1/2
Elongation at Break
50 %
50 %
50 mm/min; ISO 527-1/2
Modulus of Elasticity
2.30
GPa
334
ksi
1 mm/min; ISO 527-1/2
Flexural Strength
90.0
MPa
13100
psi
2 mm/min; ISO 178
Flexural Modulus
2.30
GPa
334
ksi
2 mm/min; ISO 178
Charpy Impact Unnotched
NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179/1eU
NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched
6.00
J/cm²
@Temperature -30.0 °C
28.6
ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
8.00
J/cm²
@Temperature 23.0 °C
38.1
ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties
Metric
English
Comments
Vicat Softening Point
109
°C
@Load 5.10 kg
228
°F
@Load 11.2 lb
50K/h; ISO 306
Flammability, UL94
HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
Processing Properties
Metric
English
Comments
Melt Temperature
240
-
260
°C
464
-
500
°F
Mold Temperature
40.0
-
80.0
°C
104
-
176
°F
Drying Temperature
80.0
°C
176
°F
Dry Time
2.00
-
6.00
hour
2.00
-
6.00
hour
Moisture Content
<= 0.020 %
<= 0.020 %
Descriptive Properties
Quality level
Virgin
DIN EN ISO 14021
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
PLMA9893 / 316521
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.