MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Covestro MONDUR® MR 5 Polyurethane
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: Mondur MR 5 is a low to medium functionality polymeric diphenylmethane diisocyanate (pMDI) containing a relatively high level of pure (monomeric) MDI.

Properties / Applications: Mondur MR 5 has a relatively high reactivity together with an extended gel time due to the high monomer content making it especially useful for microcellular and solid specialty elastomers. Mondur MR 5 also has utility in adhesive and sealants applications. As with any product, use of Mondur MR 5 in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.24 g/cc1.24 g/cc
Viscosity 50 - 95 cP50 - 95 cP
 
Thermal PropertiesMetricEnglishComments
Flash Point 203 °C397 °FPMCC
 
Descriptive Properties
Acidity<0.03%
AppearanceDark brown liquid
Content>31.8%NCO

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCOVEST0912 / 202695

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.