MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik DYNACOLL® S 1426 Copolyester
Categories: Polymer; Thermoset; Polyester, TS

Material Notes: Copolyesters: With its DYNACOLL® S product range Evonik offers thermoplastic copolyesters of high molecular weight to a wide variety of thermoplastic hot melt and solvent based applications. The individual grades differ in their melting point, degree of crystallinity and hardness and in their setting time. According to their crystallinity, the product range is arranged into four basic groups:
  • DYNACOLL® S - Highly crystalline grades
  • DYNACOLL® S - Moderately crystalline grades
  • DYNACOLL® S - Slightly crystalline grades
  • DYNACOLL® S - Amorphous grades
DYNACOLL® S copolyesters are generally supplied as granules, usually in bags of 20 or 25 kg. They can be processed into following forms of applications: adhesive film, web or net, powder, paste, hot melt and solution.

DYNACOLL® S - Amorphous grades

  • good solubility in many solvents
  • very good adhesion on a large number of substrates

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity 270 cP
@Temperature 200 °C
DIN EN ISO 3219
Viscosity Number 90 cm³/gDIN 53728
Melt Flow 15 g/10 min
@Load 2.20 kg,
Temperature 180 °C
DIN ISO 1133
 30 g/10 min
@Load 2.20 kg,
Temperature 200 °C
DIN ISO 1133
 60 g/10 min
@Load 2.20 kg,
Temperature 220 °C
DIN ISO 1133
 
Chemical PropertiesOriginal ValueComments
Total Acid Number 2.0[mg KOH/g]; DIN EN ISO 2114
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 78DIN 53505
Tensile Strength at Break 50.0 MPaDIN EN ISO 527-1/3
Elongation at Break 5.0 %DIN EN ISO 527-1/3
 
Thermal PropertiesOriginal ValueComments
Softening Point 140 °CDIN ISO 4625
Glass Transition Temp, Tg 35.0 °CDIN 53765
 
Descriptive Properties
Hydroxyl Number4 mg KOH/gDIN 53 240-02

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEVONIL102 / 196306

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.