MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
LyondellBasell Moplen HP563S Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Fiber Grade

Material Notes: Moplen HP563S is a polypropylene homopolymer manufactured using the Spheripol process. Its has excellent draw ability and spinnability properties, and is particularly suitable for production of fine denier spun bond non-wovens. Potential end use applications include diapers and sanitary napkins, apparel covers, wet tissues, shopping bags and agricultural-use textiles. Moplen HP563S can be evaluated in applications that need Anti-Gas Fading performance. Applications: Hygiene Nonwoven, Wipes/Tissues.

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccASTM D1505
Melt Flow 38 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 98ASTM D785
Tensile Strength, Yield 380 kg(f)/cm²ASTM D638
Elongation at Yield 8.0 %ASTM D638
Flexural Modulus 15000 kg(f)/cm²ASTM D790
Izod Impact, Notched 3.00 kg-cm/cm
@Temperature 23.0 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 100 °CASTM D648
 
Descriptive Properties
Processing MethodContinuous Filament/spinning, spunbond

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Avient Nanoblend™ LST 5501 Polypropylene
Avient Maxxam™ DP 4980-1-1000 Polypropylene Homopolymer (PP Homopolymer)
Avient Edgetek® ET5200-0018 UV RS Desert Sage Polypropylene Homopolymer (PP Homopolymer)
A. Schulman Diamond NPP30-2000HC Homopolymer Polypropylene
Braskem 6D43 Polypropylene Random Copolymer

PEQT9055 / 220686

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.