Hostacom ERC 198N G31325 is an 18% talc filled PP copolymer, with high melt flow, high toughness and good UV resistance. Product is available as a customized color matched, pellet form. This grade is not intended for medical, pharmaceutical, food or drinking water applications. This grade is delivered in G31325 color version. Storage at high temperatures (> 50°C) and high humidity may damage the packaging.Information provided by LyondellBasell. |