MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ChevronTexaco Havoline® MERCON®/DEXRON®-III Automatic Transmission Fluid
Categories: Fluid; Lubricant

Material Notes: Havoline Automatic Transmission Fluid MERCON/DEXRON-III delivers value through:
  • Protection against the formation of lacquers, sludge, or other harmful deposits.
  • Exceptional stability provided by excellent base oil and extra oxidation inhibitors.
  • Quiet Performance, especially effective in reducing transmission "chatter".
  • Fast circulation during cold weather and excellent lubricating body when hot.

Havoline Automatic Transmission Fluid MERCON/DEXRON-III is the latest high performance, multipurpose, pwer transmission fluit approved under Mercon® and Dexron® specifications. It is developed for passenger car and light truck automatic transmissions.

It is manufactured from select Group II base oils and additives that provide oxidation and thermal stability, friction control, load-carrying ability, corrosion and wear protection. It prevents the accumulation of deposits and the formation of sludge, varnish, and foam.

Under the most severe operating conditions, Havoline Automatic Transmission Fluid MERCON/DEXRON-III:

  • Maintains friction control for smooth shift action
  • Is specially formulated to prevent shudder
  • Retains low temperature fluidity and high temperature stability for long operating periods.
  • Protects automatic transmission fluid coolers from corrosion.
  • Practically eliminates transmission overhauls due to sludge, corrosion, wear of clutches and bands, gears and bearings, leakage past seals, and loss of frictional properties.

Havoline Automatic Transmission Fluid MERCON/DEXRON-III is designed for use in General Motors Corporation transmissions that require a DEXRON-II, DEXRON-II or DEXRON-IIE fluid, and Ford Motor Company transmissions that require a MERCON fluid. It is also used as a light oil in compressors, pumps and hydraulic systems.

  • Always check your owners manual to determine the proper automatic transmission fluid for your transmission.
  • Ford transmissions manufactured after 1996 may require a MERCON V.
  • Chrysler transmissions manufactured after 1996 require either ATF+3® or ATF+4®3.

Havoline Automatic Transmission Fluid MERCON V meets or exceeds:

  • Manufacturers performance requirements
    • Ford MERCON
    • General Motors DEXRON-III
    • Allison C4
    • Caterpillar TO-2
    • Denison P-46 Piston Pump
    • Vickers Pump
    • Voith DIWA Transmissions
    • AF transmissions

    Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.

    CPS Number: 221854; MSDS Number: 8654

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
API Gravity 32.7 °
Brookfield Viscosity 17000 cP
@Temperature -40.0 °C
Viscosity Measurement 172Viscosity Index
Saybolt Viscosity at 100°F 180 SUS
Saybolt Viscosity at 210°F 50.3 SUS
Kinematic Viscosity at 40°C (104°F) 35.5 cSt
Kinematic Viscosity at 100°C (212°F) 7.2 cSt
 
Thermal PropertiesOriginal ValueComments
Pour Point -48.0 °C
Flash Point 202 °C
 
Descriptive Properties
ColorRed

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lubriplate DEXRON III / MERCON Automatic Transmission Fluid Motor Oil & Transmission Fluid
ChevronTexaco DEXRON®-III/MERCON® Automatic Transmission Fluid
ChevronTexaco Heavy Duty Synthetic Automatic Transmission Fluid
Water, H2O
ELM® SoyFluid™ Hydraulic Universal Tractor Biodegradable Tractor Hydraulic-Transmission Fluid

WTEXA073 / 76952

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.