MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Wacker Vinnapas® 400 H Vinyl Acetate-Ethylene Copolymer
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate

Material Notes: Product description: VINNAPAS® 400 H is a poly(vinyl alcohol) stabilized vinyl acetate-ethylene copolymer dispersion with a glass transition temperature (Tg) of 0 °C. It was developed as a higher viscosity, high-performance dispersion offering a superior balance of adhesive/cohesive properties useful in achieving much higher formulation viscosities.

Properties: VINNAPAS® 400 H is used as a base for adhesives and offers a superior balance of adhesive/ cohesive properties. Much higher formulation viscosities can be achieved due to the higher viscosity of the dispersion. This allows for more dilution water to be added to achieve the same end viscosity and thus reduce overall costs. This dispersion exhibits excellent setting speed, wet tack, and high thickening response. It has clean machining and is suitable for a variety of roll, extruder or spray applications because of its poly(vinyl alcohol) stabilization. The dry film is tack-free and heat-sealable. The backbone of the polymer gives the dried adhesive film both high tensile strength and flexibility that continue to be present even with fluctuations in temperature and humidity. Just like VINNAPAS® 400, this dispersion has excellent heat resistance which, at elevated temperatures, is much greater than that exhibited by other vinyl acetate-ethylene, vinyl acetate-maleate and vinyl acetate-acrylate copolymers with similar glass transition temperatures. The initial adhesive strength is excellent even after aging, and it exhibits excellent resistance to plasticizer migration.

Application: VINNAPAS® 400 H is an excellent base for adhesive formulators and can be used in an extremely wide variety of applications. The ethylene in the polymer acts as an internal plasticizer which provides flexibility and reduces or eliminates the need for plasticizer in many applications. Because of its flexibility and excellent adhesion to so many substrates, VINNAPAS® 400 H is a versatile base in adhesives for application areas which include but are not limited to packaging (case and carton,) converting, bookbinding, textile bonding, vinyl and paper to wood laminating, automotive applications, and craft glues. It forms strong bonds between porous substrates and such films as poly(vinyl chloride) (PVC), poly(vinylidene chloride), cellulose acetate, cellophane and acrylic. VINNAPAS® 400 H adheres to widely diversified substrates such as paper, wood, cotton cloth, nylon cloth, glass and glass fibers, hardboard, urethane foam and clay coated paperboard.

Other Applications:

  • Paint (texture coatings)
  • Consumer goods
  • Gypsum board joint compound

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0379 lb/in³
Solids Content 54 - 56 %54 - 56 %
pH 4.0 - 5.54.0 - 5.5
Viscosity 3100 - 4400 cP3100 - 4400 cPdynamic
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 0.000 °C32.0 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Wacker Vinnapas® EF 104 Vinyl Acetate Ethylene
Wacker Vinnapas® EN 1165 Vinyl Acetate Ethylene
Wacker Vinnapas® 400 Vinyl Acetate-Ethylene Copolymer
LyondellBasell Hostacom EKC 430N NAT Polypropylene Copolymer, 16% Talc Filled
LyondellBasell Hifax EYG 382P C12716 Polypropylene with Glass Fiber Filler

PWACK9594 / 205123

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.