MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Skychem HY550MHS TPE, Heat resistant
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Auto parts: because of excellent (hot) oil, excellent (high temperature) bending fatigue performance, wear resistance, high strength and toughness. In the production of all kinds of elastomer parts of automobile is more excellent comprehensive performance than rubber parts, its heat resistance level higher, better low temperature properties, especially the fatigue property of TPEE is unmatched by other elastomers
Transportation: Buffers, springs; Unlike metal springs, TPEE does not rust, does not deteriorate in environmental conditions, or causes elastic breakage and loss. Compared with rubber materials, TPEE has a much greater repeatability, which can be maintained for a long period of time.
Biology and medicine: TPEE excellent performance is adjustable, has low degradation products of acidic, good biocompatibility, inflammation, not easy to induce recipient is often used in artificiality mpanic membrane, wound repair, the artificial skin, drug carrier and so on.
Plastic modification: can be used as a polymer modifier, improve, PBT, POM, PET, polystyrene (PS) engineering plastics such as low temperature performance and impact performance, improve the PC oil and resistance to stress cracking resistance, to improve the low tender soft polyvinyl chloride (PVC) and cold resistance, lower spinning temperature of polypropylene (PP), improving dyeing and feel
Textiles and shoes: Because of the unique permeability of TPEE, the water vapor in the structure can be discharged rapidly, avoiding the mold of the structure and keeping the body dry and excellent
Fiber optic communication: Because of the excellent mechanical properties, the resistance to bending can ensure that the fiber is not damaged.
Sports: Coating on skis, trail shoes sole TPEE in cold climate still has excellent performance and flexibility, impact resistance and other material has good compatibility, so can make the secondary injection molding plastic bags.
Frames: Excellent mechanical properties and wearable comfort can be used as a 3D film and television spectacle
Industrial products such as hydraulic hose and light tires: Because of TPEE long service life, good function, can be in hydraulic hose, seals, military trailer hooks, light tyres and fuel tank and a series of products in the replace pu and nylon 11 and some rubber and PVC and other plastic. The TPEE hydraulic hose remains soft below zero, while many rubber hose are inflexible. Using TPEE, the pneumatic tyre has the advantage of high strength, low quality and bending fatigue, and high load capacity without the need of reinforcement.
The design of reasonable TPEE flexible coupling, not only is the torque big, soft, hot and low, the load capacity is large, suitable for heavy machinery; And the tolerance is accurate and easy to make, superior to the TPU, metal and plastic.
In other industry, TPEE can also be used to make the lift valve, protect washer, transmission belt, tube clip, caterpillar, high pressure switch, cable sheath, switchboard insulationand shield, elastic fiber, mattress springs, roof membrane, etc.

Information provided by Shanghai Sukeyou chemical new raw materials Co., Ltd

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/ccISO 1183
Melt Flow 10 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 55ISO 868
Tensile Strength 36.0 MPaISO 527
Elongation at Break 570 %ISO 527-1
Flexural Modulus 220 MPaISO 178
 
Thermal PropertiesOriginal ValueComments
Melting Point 205 °CISO 11357
Vicat Softening Point >= 180 °CISO 306

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSKYCHEM024 / 314380

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.