MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow DOWLEX™ 2505 Linear Low Density Polyethylene, Narrow MW Distribution
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Injection Molded

Material Notes: DOWLEX® 2505 Polyethylene resin is a narrow molecular weight distribution copolymer designed to offer excellent environmental stress crack resistance and tear strength with good rigidity. It has excellent processability over a wide range of molding conditions. It complies with FDA regulation 21 CFR 177.1520 (c) 3.1(a) for food contact applications. The regulation should be consulted for complete details.

Data provided by Dow Chemical.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.926 g/cc
Viscosity 22000 cP
@Shear Rate 5000 1/s,
Temperature 190 °C
Apparent Dynamic Viscosity
 33000 cP
@Shear Rate 1000 1/s,
Temperature 190 °C
Apparent Dynamic Viscosity
 39000 cP
@Shear Rate 300 1/s,
Temperature 190 °C
Apparent Dynamic Viscosity
Melt Flow 85 g/10 min
@Load 2.16 kg
Melt flow ratio I10/I2 is 6.4.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 8.55 MPa
Tensile Strength, Yield 9.60 MPa
Elongation at Break 640 %
Modulus of Elasticity 0.219 GPaMolded Sample 2% Secant Modulus
Flexural Modulus 0.356 GPa
Izod Impact, Notched (ISO) 39.0 kJ/m²
@Temperature -50.0 °C
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 93.0 °C
 
Compliance PropertiesOriginal ValueComments
FDA Yes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow DNDA-9810 NT 7 Linear Low Density Polyethylene Resin
Dow DOWLEX™ 2500 Linear Low Density Polyethylene, Narrow MW Distribution
Braskem IF33 LLDPE Injection Molding Polyethylene Copolymer
Dow DOWLEX™ 2503 Linear Low Density Polyethylene, Narrow MW Distribution
Dow DOWLEX™ 2503.10 Linear Low Density Polyethylene, Narrow MW Distribution

PDW451 / 34520

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.