MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Geon® Performance Solutions Vinyl Dry Blend E7857 PVC, Rigid  (discontinued **)
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, High Impact; PVC, Rigid Grade

Material Notes: The Cell Classification was determined using the notched Izod test with injection molded samples.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.46 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 83
@Time 15.0 sec
ASTM D2240
Tensile Strength, Yield 42.7 MPaType I, 5.1 mm/min; ASTM D638
Tensile Modulus 2450 MPaType I, 5.1 mm/min; ASTM D638
Flexural Strength 77.9 MPaASTM D790
Flexural Modulus 2830 MPaASTM D790
Izod Impact, Notched 203 J/m
@Thickness 3.18 mm,
Temperature 23.0 °C
Across Flow, Compression Molded; ASTM D256A
 219 J/m
@Thickness 3.18 mm,
Temperature 23.0 °C
Flow, Compression Molded; ASTM D256A
 1260 J/m
@Thickness 3.18 mm,
Temperature 23.0 °C
Injection Molded; ASTM D256A
Dart Drop Total Energy 53.4 J/cm
@Temperature 23.0 °C
Procedure A, C.125 Dart; ASTM D4226
 187 J/cm
@Temperature 23.0 °C
Procedure B, C.125 Dart; ASTM D4226
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 59.0 µm/m-°CASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 72.8 °C
@Thickness 3.18 mm
Unannealed; ASTM D648
 
Processing PropertiesOriginal ValueComments
Melt Temperature 182 - 193 °C
 
Descriptive Properties
Ease of SizingGood
FeaturesGood Weather Resistance
 High Impact Resistance
FormsPowder
Processing MethodExtrusion
PVC Cell Classification1-41432-33ASTM D4216
 16334ASTM D1784
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
UsesOutdoor Applications
 Profiles
 Windows & Doors

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
GEHR Plastics PVC-HI Polyvinylchloride, Impact Grade
Novatec Novablend® 6701 PVC
Hippe PA 46 Nylon 46
Overview of materials for Polypropylene, Glass/Mineral Reinforced
Overview of materials for Polypropylene, Glass Reinforced, Impact Modified

PH1PN8269 / 102105

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.