MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Unifrax Fiberfrax® LDS Moldable Moldable Insulation
Categories: Ceramic

Material Notes: Fiberfrax LDS and LDS-AL moldables consist of Fiberfrax ceramic fibers dispersed in a sticky water-based refractory binder. These materials have a putty-like consistency which permits application by caulking, troweling, or hand forming. Both products adhere well to most surfaces. Drying is accomplished at a noncritical, elevated temperature, and the resulting dried material is strong, hard, and erosion resistant. LDS-AL moldable possesses excellent resistance to wetting by many nonferrous molten metals and is used extensively in molten aluminum contact applications.

    Typical Applications
  • Patch refractory joints and cracks
  • Hardware protection of ceramic fiber furnace linings
  • Patch around burner blocks
  • Refractory backup

Information Provided by Unifrax I LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 50.0 lb/ft³Dry
 85.0 lb/ft³Wet
Solids Content 55 %
Loss On Ignition 5.0 %
 
Mechanical PropertiesOriginal ValueComments
Modulus of Rupture 0.400 ksiDry
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 1093 °CRecommended Operating Temperature
Shrinkage 4.0 %
@Temperature 1090 °C,
Time 86400 sec
 
Descriptive Properties
AppearanceSticky putty
Molten Aluminum Wetting ResistanceGood
Temperature Grade (°F)2300

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ultramid® T 4381 LDS 10/25% Glass/Mineral Filled PA6/6T (Conditioned)
RTP Company RTP 3499-3 X 113393 C Liquid Crystal Polymer (LCP) Glass Fiber - LDS Platable
Mitsubishi Xantar® LDS 3760 Polycarbonate
EPICHEM Epilon G2-PC 10% GF Polycarbonate, 10% Glass Fiber

CUNIF045 / 97817

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.