MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Teknor Apex Sarlink® TPE ME-2242D-01 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Sarlink ME-2242D-01 is a general purpose thermoplastic elastomer used in automotive applications, including exterior. Sarlink ME-2242D-01 is a high hardness, low density grade exhibiting superior chemical resistance. This grade can be processed by injection molding.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Features: Abrasion Resistant; Anti-fogging; Bondability; Chemical Resistant; General Purpose; Good Adhesion; Good Color Stability; Good Colorability; Good Flow; Good Moldability; Good Processability; Good Scratch Resistance; Good Tear Strength; Low Density; Low Gloss; Low Temperature Impact Resistance; Lubricated; Paintable; Pleasing Surface Appearance; Slip; UV Resistant; Wear Resistant; Without Fillers

Uses: Automotive Applications; Automotive Exterior Parts; ; Automotive Exterior Trim; Automotive Interior Parts; Automotive Interior Trim; Overmolding; Rubber Replacement

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Injection Molding

Preliminary data. Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.916 g/ccISO 1183
Viscosity 451 cP
@Shear Rate 206 1/s,
Temperature 200 °C
ASTM D3835
Melt Flow 5.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 40
@Time 15.0 sec
Injection Molded; ISO 868
 42
@Time 5.00 sec
Injection Molded; ISO 868
 45
@Time 1.00 sec
Injection Molded; ISO 868
 43.5
@Treatment Temp. 100 °C,
Time 15.0 sec
Change in Air, 1000 hr; ISO 888
 47.9
@Treatment Temp. 100 °C,
Time 5.00 sec
Change in Air, 1000 hr; ISO 888
 51.2
@Treatment Temp. 100 °C,
Time 1.00 sec
Change in Air, 1000 hr; ISO 888
Tensile Strength at Break 1160 psiAcross Flow, Type 1, 20 in/min; ISO 37
 1500 psiFlow, Type 1, 20 in/min; ISO 37
 1230 psi
@Treatment Temp. 100 °C,
Time 3.60e+6 sec
Across Flow, Type 1, Change in Air, 1000 hr; ISO 188
 1580 psi
@Treatment Temp. 100 °C,
Time 3.60e+6 sec
Flow, Type 1, Change in Air, 1000 hr; ISO 188
Tensile Stress at Strain 1060 psi
@Strain 100 %
Across Flow, Type 1, 20 in/min; ISO 37
 1400 psi
@Strain 100 %
Flow, Type 1, 20 in/min; ISO 37
 1190 psi
@Strain 100 %,
Treatment Temp. 100 °C
Across Flow, Type 1, Change in Air, 1000 hr; ISO 188
 1550 psi
@Strain 100 %,
Treatment Temp. 100 °C
Flow, Type 1, Change in Air, 1000 hr; ISO 188
Elongation at Break 440 %Flow, Type 1, 20 in/min; ISO 37
 530 %Across Flow, Type 1, 20 in/min; ISO 37
 246 %
@Treatment Temp. 100 °C,
Time 3.60e+6 sec
Flow, Type 1, Change in Air, 1000 hr; ISO 188
 307 %
@Treatment Temp. 100 °C,
Time 3.60e+6 sec
Across Flow, Type 1, Change in Air, 1000 hr; ISO 188
Flexural Yield Strength 1230 psi
@Strain 5.0 %
ISO 178
Flexural Modulus 52400 psiISO 178
Tear Strength 360 pliFlow, Method Ba, Angle (Unnicked), 20 in/min; ISO 34-1
 440 pliAcross Flow, Method Ba, Angle (Unnicked), 20 in/min; ISO 34-1
Compression Set 64 %
@Temperature 22.8 °C,
Time 79200 sec
Type 1; ISO 815
 80 %
@Temperature 70.0 °C,
Time 79200 sec
Type 1; ISO 815
 99 %
@Temperature 90.0 °C,
Time 252000 sec
Type 1; ISO 815
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 420 - 460 °F
Middle Barrel Temperature 420 - 460 °F
Front Barrel Temperature 420 - 460 °F
Nozzle Temperature 420 - 460 °F
Melt Temperature 420 - 460 °F
Mold Temperature 60.0 - 90.0 °F
Injection Pressure 200 - 1000 psi
Back Pressure 25.0 - 125 psi
Cushion 0.150 - 1.00 in
Screw Speed 50 - 120 rpm
 
Descriptive Properties
AppearanceColors Available
 Natural Color
 Translucent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTEKNQ1058 / 237549

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.